| 涂盐热腐蚀环境中GH37合金的蠕变断裂 |
| 林栋樑;黄伟;张源虎 |
| 上海交通大学;上海交通大学;上海交通大学 |
|
| CREEP RUPTURE BEHAVIOUR OF SALT-COATED SUPERALLOY GH37 IN A HOT ENVIRONMENT |
| by LIN Dongliang (T. L. Lin); HUANG Wei; ZHANG Yuanghu (Shanghai Jiaotong University)(Manuscript received 3 May; 1986; revised manuscript 28 July; 1986) |
引用本文:
林栋樑;黄伟;张源虎. 涂盐热腐蚀环境中GH37合金的蠕变断裂[J]. 金属学报, 1987, 23(5): 413-420.
,
,
.
CREEP RUPTURE BEHAVIOUR OF SALT-COATED SUPERALLOY GH37 IN A HOT ENVIRONMENT[J]. Acta Metall Sin, 1987, 23(5): 413-420.
1 Lin T L, Zhang Y H, Yang H W. Mater Sci Eng, 1984; 62: 17 2 Guo JT (郭建亭), Ranucci D, Picco E, Strocchi P M. In: Brunetaud R et at eds., High Temperature Alloys For Gas Turbines, Dordrecht R Neth: D. Reidel, 1982: 805 3 魏翔云,郝惠清,肖耀天.金属学报,1984;20:A365 4 吉蕖正行,宫川大诲,坂本庸晃,藤代大,铁钢,1982;68:120 5 Nicholls J R, Samnal J, Hurst R C, Hancock P. In: Kirman I et al eds., Behaviour of High Temperature Alloys in Aggressive Environment, Proc Pettern Int Conf, Londou: The Metal Soc, 1980: 911 6 Tien J K, Davidson J M. In: Fontana M G, Steahle R W eds., Corrosion Science and Technology, vol. 7, New york and London; Plenum, 1976: 1 7 张源虎,胡赓祥.机械工程材料,1985;9(1) :13 8 Mrowec S. In: Proc 8th Int Conf on Metallic Corrosion of Mainz, Frankfurt am Main: DECHEMA Deutsche Gesellschaft fur Chemisches Apparatewesen, 1981: 2110# |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|