| 过载对疲劳裂纹低速扩展的影响 |
| 邓蓉英 |
| 中国科学院力学研究所 |
|
| EFFECT OF OVERLOAD ON FATIGUE CRACK PROPAGATION NEAR THRESHOLD |
| by DENG Rongying (Institute of Mechanics; Academia Sinica; Beijing)(Manuscript received 12 May; 1986; revised manuscript 22 August; 1986) |
引用本文:
邓蓉英. 过载对疲劳裂纹低速扩展的影响[J]. 金属学报, 1987, 23(5): 421-424.
.
EFFECT OF OVERLOAD ON FATIGUE CRACK PROPAGATION NEAR THRESHOLD[J]. Acta Metall Sin, 1987, 23(5): 421-424.
1 Jones R E. Eng Fract Mech, 1973; 5: 585 2 Matsuoka S, Tanaka K. Eng Fract Mech, 1978; 10: 515 3 Bathias C, Vancon M. Eng Fract Mech, 1978; 10: 409 4 邓蓉英,于桂清,李禾.金属学报,1986;22:A409 5 Elber W.ASTM, STP 486, 1971: 230 6 Schijve J. Rep Mp 195, National Luchtvaart Laloratorium Amsterdam, 1960b |
|