    					| 含铌铁水-铌渣的平衡和渣中α_(Nb_2O_5)的测定 | 
  					 
  					  										
						| 陈伟庆;周荣章;林宗彩 | 
					 
															
					| 北京钢铁学院;北京钢铁学院;北京钢铁学院 | 
					 
										
						 | 
					 
   										
    					| THE INVESTIGATION OF EQUILIBRIUM BETWEEN SLAG AND HOT METAL CONTAINING Nb AND MEASUREMENT OF αNb_2O_5 IN THE SLAG | 
  					 
  					  					  					
						| by CHEN Weiqing; ZHOU Rongzhang; LIN Zongcai (Beijing University of Iron and Steel Technology) (Manuscript received 6 June; 1986; revised manuscript 6 October; 1986) | 
					 
														 
				
				引用本文: 
				
								陈伟庆;周荣章;林宗彩. 含铌铁水-铌渣的平衡和渣中α_(Nb_2O_5)的测定[J]. 金属学报, 1987, 23(6): 560-567.	
																												 																				 ,
																								 ,
																												 . 
				THE INVESTIGATION OF EQUILIBRIUM BETWEEN SLAG AND HOT METAL CONTAINING Nb AND MEASUREMENT OF αNb_2O_5 IN THE SLAG[J]. Acta Metall Sin, 1987, 23(6): 560-567.	                                                        				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
                         
            
									            
									                
																														  
																|  1 福沢章.钢铁,1984;19(8) :56
2 陈伟庆,周荣章,林宗彩.钢铁,1987;22(5) :7
3 Schmalzried H. Ber Bunsenges Phys Chem, 1962; 66: 572
4 Elliott J F. Thermochemistry for Steeimaking, Vol. Ⅱ, Mass: Addison-Wesley, 1963
5 Janke D, Fischer W A. Arch Eisenhuettenwes, 1975; 46: 755
6 郭上型,唐仲和,张永定.全国第五届冶金物化年会论文集(上册),1984:157
7 罗晨,苏良赫.包钢含铌炼钢渣工业岩石学研究,武汉地质学院北京研究生部研究生论文,1983
8 Sigworth G K, Elliott J F. Met Sci, 1974; 8: 298
9 魏寿昆,张圣弼,佟亭,谭赞麟,钢铁.1984;19(7) :1
10 Schenck H, Steinmetz E. Wirkungsparameter Von Beglcitelementen flussiger Eisenloesungen und ihre gegenseitigen Beziehungen, Duesseldorf: Stahleisen-Sonderberichte, 1968: 39
11 日本铁钢学会.铁钢便霓,Ⅰ基礎,表1,3,第3版,东京:丸善,1981:22
12 张圣弼,佟亭,王济舫,魏寿昆.金属学报,1984;20:A 348
13 董元篪,彭(忄育)强,李丽芬,朱元凯,魏寿昆.全国第五届冶金物化年会论文集(上册),1984:217 | 
															   
																													 
									             
									           
             
			            			 
			 
             
												
											    	
											        	 | 
											        	Viewed | 
											         
													
											        	 | 
											        	 | 
											         
											      	
												         | 
												        
												        	Full text 
												          	
												         | 
											        	
												        	
												        	 
												        	
												          	 
												          	
												          	
														 | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        
												        	Abstract 
												          	
														 | 
												        
															
															 
															
															
												         | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        Cited  | 
												        
												        	
												         | 
													 
													
												         | 
												         | 
												         | 
													 
													
													    |   | 
													    Shared | 
													       | 
												  	 
												  	
													     | 
													     | 
													     | 
											  		 
											  		
													    |   | 
													    Discussed | 
													       | 
												  	 
											 
											 
             
           
      
									
									
		
									
									
									
									
									
									 | 
								 
							 
						 | 
					 
				 
			
		 |