| (Ⅰ+Ⅱ)复合型氢致开裂的研究 |
| 高桦;薛礼觉 |
| 上海工程技术大学材料系;上海工程技术大学 |
|
| (I+II) MIXED MODE HYDROGEN INDUCED CRACKING |
| GAO Hua;XUE Lijue Shanghai University of Engineerin Science |
引用本文:
高桦;薛礼觉. (Ⅰ+Ⅱ)复合型氢致开裂的研究[J]. 金属学报, 1989, 25(1): 48-52.
,
.
(I+II) MIXED MODE HYDROGEN INDUCED CRACKING[J]. Acta Metall Sin, 1989, 25(1): 48-52.
| 1 John C St, Gerberich W W. Metall Trans, 1973; 4: 589--594
2 John C F St. Scr Metall, 1975; 9: 141
3 McGuinn K F, Aballe M. Br Corros J, 1982; 17: 18
4 Pickens J R, Gordon J R, Green J A S. Metall Trans, 1983; 14A: 925
5 Nichols F A. Corrosion, 1983; 39: 449--451
6 张统一,褚武扬,李英,肖纪美.金属学报,1986;22:A349
7 高桦,王自强,杨成寿,周爱华.金属学报.1979;15:A380
8 Gao Hua, Brown M W, Miller K J. Fatigue Eng Mater Struct, 1982; 5: 1
9 Erdogan F, Sih G C. J Basic Eng, 1963; 85: 519
10 朱日彰,童建筑,张文奇.中国腐蚀与防护学报,1986;6:42 |
|