| 疲劳软化的低能位错结构 |
| 柴惠芬;汪立勤;C.LAIRD |
| 西安交通大学;西安交通大学;UniversityofPennsylvania |
|
| LOW ENERGY DISLOCATION STRUCTURES DUE TO FATIGUE SOFTENING |
| CHAI Huifen;WANG Liqin;C. LAIRD Xi'an Jiaotong University University of Pennsylvania; U. S. A |
引用本文:
柴惠芬;汪立勤;C.LAIRD. 疲劳软化的低能位错结构[J]. 金属学报, 1989, 25(3): 45-50.
,
,
.
LOW ENERGY DISLOCATION STRUCTURES DUE TO FATIGUE SOFTENING[J]. Acta Metall Sin, 1989, 25(3): 45-50.
1 Ramaswami B, Lau T W F. Mater Sci Eng, 1980; 46: 221 2 Kuhlmann-Wilsdorf D. Metall Trans, 1985; 16A: 2091 3 Chai Huifen (柴惠芬), Laird C. Mater Sci Eng, 1987; 93: 159 4 Foxall R A, Duesbery M S, Hitsch P B. Can J Phys, 1967; 45: 607 5 Kuhlmann-Wilsdorf D. In: Thompson A W ed, Workhardening in Tension and Fatigue. AIME, 1977: 1 6 Ackermann F, Kubin L P, Lepinoux J, Mughrabi H. Acta Metall, 1984; 32: 715 7 Charsley P. Mater Sci Eng, 1981; 47: 181 8 Jin N Y, Winter A T. Acta Metall, 1984; 32: 1173 9 Dickson J I, Boutin J, Lesperance G. Acta Metall, 1986; 34: 150 |
|