| 微量B、Ga对Mn-Si-Cr热轧双相钢转变控制的影响 |
| 何泽福;刘天模;吴允建 |
| 重庆大学;重庆大学;重庆大学 |
|
| EFFECT OF TRACE B AND Ga ON TRANSFORMATION CONTROL OF Mn-Si-Cr AS-ROLLED DUAL PHASE STEELS |
| HE Zefu;LIU Tianmo;WU Yunjian Chongqing University |
引用本文:
何泽福;刘天模;吴允建. 微量B、Ga对Mn-Si-Cr热轧双相钢转变控制的影响[J]. 金属学报, 1989, 25(3): 73-75.
,
,
.
EFFECT OF TRACE B AND Ga ON TRANSFORMATION CONTROL OF Mn-Si-Cr AS-ROLLED DUAL PHASE STEELS[J]. Acta Metall Sin, 1989, 25(3): 73-75.
1 花井谕,渡辺国男,江坂一彬.铁钢,1982;68:1306 2 Barr R Q. Alloys for the Eighties, Connecticut: Climax Molybdenum Company, 1978: 37 3 马鸣图,吴宝榕.国外金属材料,1982;(10) : 9 4 何泽福,夏进,钱小蓉.重庆大学学报,1985;(1) : 83 5 Coldren A P, Eldis G T. J Met, 1980; 32(3) : 41 6 刘富国,黄文轩,何泽福.钢铁钒钛,1982;(3) :1 7 Kubaschewki O. Iron-Binary Phase Diagrams, Berlin: Springer-Verlag, 1982: 38 |
|