| Cu-Dy-Ni(Dy≤35wt-%)三元合金系相图的室温截面 |
| 李德萱;郑建宣 |
| 广西大学;广西大学 |
|
| ROOM TEMPERATURE SECTION OF Cu-Dy(≤35wt-%)-Ni TERNARY PHASE DIAGRAM |
| LI Dexuan;ZHENG Jianxuan Guangxi University; Nanning |
引用本文:
李德萱;郑建宣. Cu-Dy-Ni(Dy≤35wt-%)三元合金系相图的室温截面[J]. 金属学报, 1989, 25(3): 134-136.
,
.
ROOM TEMPERATURE SECTION OF Cu-Dy(≤35wt-%)-Ni TERNARY PHASE DIAGRAM[J]. Acta Metall Sin, 1989, 25(3): 134-136.
1 郑建宣,王淳正.物理学报,1982;31:669--672 2 郑建宣,徐国雄.物理学报,1982;31:807--809 3 Smithells C J. Metals Reference Book, 5th ed., London: Butterworth, 1976: 586 4 Buschow K H J, Van Der Goot A S. Acta Crystallogr, Ser. B, 1971; 27: 1085 5 王淳正,郑建宣.金属学报,1985;21:B62--65a |
|