| 不同因素对连铸机中间包流场的影响 |
| 贺友多;Y.SAHAI |
| 包头钢铁学院;美国俄亥俄州立大学 |
|
| INFLUENCE OF SOME FACTORS ON FLUID FLOW IN CONTINUOUS CASTING TUNDISHES |
| HE Youduo;Y. SAHAI Baotou Institute of Iron & Steel Technology The Ohio State University |
引用本文:
贺友多;Y.SAHAI. 不同因素对连铸机中间包流场的影响[J]. 金属学报, 1989, 25(4): 132-136.
,
.
INFLUENCE OF SOME FACTORS ON FLUID FLOW IN CONTINUOUS CASTING TUNDISHES[J]. Acta Metall Sin, 1989, 25(4): 132-136.
1 贺友多,Sahai Y.金属学报,1988;24:B79--86 2 Launder B E, Spalding D B. Comput Method Appl Mech Eng, 1974; 3: 269 3 Launder B E, Spalding D B. Heat Transfer Section Report, No. HTS/73/2, Imperial College, London, 1973 4 王应时,范维澄,周力行,徐旭常.燃烧过程数值计算,北京:科学出版社,1986 5 窦国仁.紊流力学,北京:人民教育出版社,1984 6 陈景仁.流体力学及传热学,北京:国防工业出版社,1984 7 Hinze J O. Turbulence, New York: McGraw-Hill, 1959 8 Gosman A D, Launder B E. TEACH-2E, Internal Report, Mech Eng Dept, Imperial College, London, 1976 9 He Y, Sahai Y. Metal Trans, 1987; 18B: 81--92 10 Patanker S V. Numerical Heat Transfer and Fluid Flow, New York: McGraw-Hill, 1980 11 Sahai Y, Guthrie R I L. Metal Trans, 1982; 13B: 193--202 12 Sahai Y, Guthrie R I L. Metal Trans, 1982; 13B: 203--210 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|