| ZG15CrMoV和35钢在500—1400℃下的流变行为 |
| 徐东;安阁英;李庆春 |
| 上海交通大学;哈尔滨工业大学;哈尔滨工业大学 |
|
| RHEOLOGICAL BEHAVIOUR OF STEELS ZG15CrMoV AND 35 IN TEMPERATURE RANGE OF 500--1400℃ |
| XU Dong;AN Geying;LI Qingchun Shanghai Jiaotong University; Harbin Institute of Technology |
引用本文:
徐东;安阁英;李庆春. ZG15CrMoV和35钢在500—1400℃下的流变行为[J]. 金属学报, 1992, 28(3): 81-86.
,
,
.
RHEOLOGICAL BEHAVIOUR OF STEELS ZG15CrMoV AND 35 IN TEMPERATURE RANGE OF 500--1400℃[J]. Acta Metall Sin, 1992, 28(3): 81-86.