焊接接头特征区的能谱分析与隶属函数 |
王嘉玲 |
太原工业大学 |
|
ENERGY SPECTRUM ANALYSIS AND MEMBERSHIP FUNCTION OF PROPERTY REGION OF WELDING JOINT |
WANG Jialing(Taiyuan University of Technology)(Manuscript received 22 July;1993;in revised form 4 October;1993) |
引用本文:
王嘉玲. 焊接接头特征区的能谱分析与隶属函数[J]. 金属学报, 1994, 30(16): 175-179.
.
ENERGY SPECTRUM ANALYSIS AND MEMBERSHIP FUNCTION OF PROPERTY REGION OF WELDING JOINT[J]. Acta Metall Sin, 1994, 30(16): 175-179.
1SavageWF.WeldRes,1976;2602王善元.焊接金相实用讲义.哈尔滨焊接研究所,1983:1123周振丰,张文铖.焊接冶金及金属焊接性.北京:机械工业出版社,1987:1054陈伯蠡.金属焊接性基础.北京:机械工业出版社,1983:945汪培庄.模糊集合论及其应用.上海科学技术出版社,1983:256邹开其,靳正大.模糊数学方法.大连海运学院出版社,1990:15$ |
|