焊接接头特征区的能谱分析与隶属函数
王嘉玲
太原工业大学
ENERGY SPECTRUM ANALYSIS AND MEMBERSHIP FUNCTION OF PROPERTY REGION OF WELDING JOINT
WANG Jialing(Taiyuan University of Technology)(Manuscript received 22 July;1993;in revised form 4 October;1993)
引用本文:

王嘉玲. 焊接接头特征区的能谱分析与隶属函数[J]. 金属学报, 1994, 30(16): 175-179.
. ENERGY SPECTRUM ANALYSIS AND MEMBERSHIP FUNCTION OF PROPERTY REGION OF WELDING JOINT[J]. Acta Metall Sin, 1994, 30(16): 175-179.

全文: PDF(298 KB)  
摘要: 用电子扫描能谱分析和隶属函数分析了熔化焊接接头特征区,结果表明,这种方法能确定焊接接头的特征区,并为检验金相组织和判定级别等提供理论依据.
关键词 : 焊接接头特征区,  电子扫描能谱分析,  隶属函数,  金相组织    
Abstract:Scanning electron spectroscopic analysis and membership function have been adopted to determine reliably the property region of welding joint and to furnish theoretical evidence for examination of microstructure and decision of grade.Correspondent:WANG Jialing,Faculty of Welding,(Department of Materials,Taiyuan University of Technology,Taiyuan 030024)
Key words: property region of welding joint    scanning electron spectroscopic analysis    membership function    microstructure
    
1SavageWF.WeldRes,1976;2602王善元.焊接金相实用讲义.哈尔滨焊接研究所,1983:1123周振丰,张文铖.焊接冶金及金属焊接性.北京:机械工业出版社,1987:1054陈伯蠡.金属焊接性基础.北京:机械工业出版社,1983:945汪培庄.模糊集合论及其应用.上海科学技术出版社,1983:256邹开其,靳正大.模糊数学方法.大连海运学院出版社,1990:15$