TiNi形状记忆合金中的亚稳相 |
赵兴中;吴杏芳;柯俊 |
北京科技大学;华中理工大学材料科学与工程系金属材料教研室 |
|
METASTABLE x-PHASE IN TiNi SHAPE MEMORY ALLOY |
ZHAO Xingzhong; WU Xingfang; KE Jun (University of Science and Technology Beijing)(Manuscript received 18 June; 1993; in revised form 29 November; 1993) |
引用本文:
赵兴中;吴杏芳;柯俊. TiNi形状记忆合金中的亚稳相[J]. 金属学报, 1994, 30(7): 302-306.
,
,
.
METASTABLE x-PHASE IN TiNi SHAPE MEMORY ALLOY[J]. Acta Metall Sin, 1994, 30(7): 302-306.