金属学报  2020, Vol. 56 Issue (1): 83-98    DOI: 10.11900/0412.1961.2019.00053
  综述 本期目录 | 过刊浏览 |
电弧增减材复合制造精度控制研究进展
卢振洋1,2,田宏宇1,3,陈树君1(),李方1
1. 北京工业大学汽车结构部件先进制造技术教育部工程研究中心 北京 100124
2. 北京联合大学机器人学院 北京 100101
3. 北京市智能机械创新设计服务工程技术研究中心 北京 100020
Review on Precision Control Technologies of Additive Manufacturing Hybrid Subtractive Process
LU Zhenyang1,2,TIAN Hongyu1,3,CHEN Shujun1(),LI Fang1
1. Engineering Research Center of Advanced Manufacturing Technology for Automotive Components-Ministry of Education, Beijing University of Technology, Beijing 100124, China
2. College of Robotics, Beijing Union University, Beijing 100101, China
3. Beijing Engineering Research Center of Smart Mechanical Innovation Design Service, Beijing 100020, China
引用本文:

卢振洋,田宏宇,陈树君,李方. 电弧增减材复合制造精度控制研究进展[J]. 金属学报, 2020, 56(1): 83-98.
Zhenyang LU, Hongyu TIAN, Shujun CHEN, Fang LI. Review on Precision Control Technologies of Additive Manufacturing Hybrid Subtractive Process[J]. Acta Metall Sin, 2020, 56(1): 83-98.

全文: PDF(23268 KB)   HTML
摘要: 

电弧增减材复合制造技术是一种将产品设计、软件控制以及增材制造与减材制造相结合的新兴技术。丝材电弧增材制造(WAAM),因其在金属增材制造中具有制备成本低、沉积效率高、材料利用率高等优势而备受推崇;又因其热输入高、成型精度相对较低而存在一定局限性。因此,亟待研发既能保证成形效率,又可以精确控制传热、传质、传力的增材复合制造技术。电弧增减材复合制造对于大型框架构件上肋板或类似薄壁墙体、筋板等构件的加工十分适合,可以实现降低制造成本和提高生产效率的目的。除增材制造精度和应力控制等问题外,增材后控形减材制造的切削问题不同于传统的去除加工,也受增材沉积表面不均匀性、增材余热和残余应力等因素影响。为解决上述问题,近年来为实现高速高效成形、精确控形控性的多种增减材复合制造方法不断涌现。本文对目前增材制造成形误差、增材后应力变形控制,以及增材后减材切削加工的相关研究进行综述,旨在探索金属构件增材复合带温减材制造的可行性,寻求合理利用增材余热,在保证最佳加工精度的前提下追求较小残余应力、良好材料微观性能和较高生产率的新型制造工艺。

关键词 : 电弧丝材增材制造,  复合制造,  精度控制    
Abstract:

A hybrid technique of additive manufacturing and subtractive process has provided a new solution combining product design and control by software. Wire arc additive manufacturing (WAAM) process wins well-respected because of its low cost and high efficiency of deposition, nevertheless the process has its limitation of high heat input and low forming accuracy. A new process of additive manufacturing with high efficiency of modeling is urgent needed which can control heat transfer, mass transfer and force transfer. To overcome the disadvantage upon, various hybrid manufacturing techniques have been developed with high efficiency and controlled modeling in recently. The machining process in hybrid manufacturing has more different characteristics from traditional material removal processes, such as residual stress and heat in the blank. These influence the whole efficiency of the hybrid manufacturing. The primary aim of this paper is to explore the feasibility of thermal machining during this process and make rational use of additive manufacturing in order to obtain optimal accuracy.

Key words: wire arc additive manufacturing    hybrid manufacturing process    precision control
收稿日期: 2019-02-28     
ZTFLH:  TG409  
基金资助:国家自然科学基金项目(51475008);国家自然科学基金项目(51775007);中国博士后科学基金项目(2017M610726);国家科技重大专项项目(2014ZX04001-171)
作者简介: 卢振洋,男,1957年生,教授,博士
图1  丝材电弧增材制造原理图
图2  电弧增材制造案例[10]
图3  NTi公司电弧增材制造案例及加工后成品[10]
图4  整体壁板结构及其制造流程对比[11]
图5  电弧增材复合铣削减材制造中误差传递示意图[11]
图6  电弧增材制造中扰动因素[1,13,14,15]
图7  拐角和圆弧处成形形貌误差[19]
图8  成形形貌随沉积高度的变化规律[25]
图9  旁路电弧控制工艺原理图[32]

Method

Welding heat sourceMaterial typeWorking condition

Dimension

Efficiency

Forming precisionPost processing
SLMLaserPowderInert gasMedium-sizedMedium-lowHighLess
EBSMElectron beamPowderVacuumMedium-sizedMedium-lowHighLess
LSFLaserPowderInert gasMedium-sizedMedium-lowHighLess
WAAMWelding arcWireOpenLargeHighLowMore
表1  几种常见金属增材制造技术对比
SortTechnical principleLimitation
Surface tension transition (STT)To improve the energy accumulation of droplets, the welding current can be reduced instantaneously and the spatter can be effectively reduced before the droplet short circuit liquid bridge bursts

Short-circuit transition is required and robustness is insufficient

Pulse GMAWImproving droplet energy accumulation, peak current transfer droplet and base dimension arc, reducing average heat inputThe thermal input of the peak value of pulse impacts the substrate

Droplet excitation

Improving droplet energy accumulation, using droplet oscillation inertia force to promote droplet transition, reducing pulse peak current and improving transition robustness

Precise matching of droplet oscillation phase is required

Cold metal transfer (CMT)

By introducing mechanical force, the welding wire can be fed back and forth, the short-circuit droplets can be broken mechanically, there is no spatter transition, and the heat input is low

The dynamic performance of the motor is limited, and the torch is complex and bulky

Magnetic control GMAW

The external magnetic field is introduced to add Lorentz force to increase the transition frequency

The effect is weak

Bypass GMAWBy introducing the bypass arc with additional electromagnetic force, the droplet transition can be significantly promotedMulti-electrode accessibility is limited, high arc length avoids arcing

Ultrasonic GMAW

Welding arc space composites ultrasonic field, while the ultrasonic radiation force promotes the droplet transition and the droplet transition is often under the longer arc

Droplet size can be controlled, but it is difficult to provide directivity

Laser enhancement GMAW

Laser evaporation reaction is introduced. Pulsed laser irradiates droplets. Laser impulse promotes droplet detachment and realizes controllable transition

The direction of evaporation reaction force is directly related to the surface morphology of droplets, so it is difficult to accurately control the direction of force
表2  电弧热源熔滴过渡控制的成果
图10  电弧增减材复合制造软件系统及其零件[18]
图11  固有应变法等效模型[48]
图12  增减材复合制造中的变形-应力联合数值仿真[55]
[1] Li F, Chen S J, Wu Z Y, et al. Adaptive process control of wire and arc additive manufacturing for fabricating complex-shaped components [J]. Int. J. Adv. Manuf. Technol., 2018, 96: 871
[2] Li F, Chen S J, Shi J B, et al. Investigation on surface quality in a hybrid manufacturing system combining wire and arc additive manufacturing and machining [A]. Transactions on Intelligent Welding Manufacturing [C]. Singapore: Springer, 2018: 127
[3] Karunakaran K P, Suryakumar S, Pushpa V, et al. Low cost integration of additive and subtractive processes for hybrid layered manufacturing [J]. Robot. Comput. -Integr. Manuf., 2010, 26: 490
[4] Tian C L, Chen J L, Dong P, et al. Current state and future development of the wire arc additive manufacture technology abroad [J]. Aerospace Manuf. Technol., 2015, (2): 57
[4] (田彩兰, 陈济轮, 董 鹏等. 国外电弧增材制造技术的研究现状及展望 [J]. 航天制造技术, 2015, (2): 57)
[5] Zhang R. Research on the aluminum alloy arc additive manufacturing (3D printing) technology and process based on the CMT [D]. Nanjing: Nanjing University of Science & Technology, 2016
[5] (张 瑞. 基于CMT的铝合金电弧增材制造(3D打印)技术及工艺研究 [D]. 南京: 南京理工大学, 2016)
[6] Zhang Y, Wu T M, Tang H Y, et al. Research on a multifunctional five axis metal intelligent equipment hybrid additive and subtractive manufacturing with high speed and efficiency [J]. Int. Combust. Engine Parts, 2018, (3): 115
[6] (张 宇, 吴天明, 唐鸿雁等. 多功能高速高效五轴金属增减材复合智能装备研制 [J]. 内燃机与配件, 2018, (3): 115)
[7] Du W, Bai Q, Zhang B. A novel method for additive/subtractive hybrid manufacturing of metallic parts [J]. Proced. Manuf., 2016, 5: 1018
[8] Xia R F, Fan J X, Li X Y, et al. Research on a hybrid machining system and process based on wire arc additive manufacturing and milling [J]. Manuf. Autom., 2016, 38(9): 79
[8] (夏然飞, 樊建勋, 李新宇等. 电弧增材制造与铣削复合加工系统与工艺研究 [J]. 制造业自动化, 2016, 38(9): 79)
[9] Sun C S, Zhang Z D, Liu L M. Microstructure and mechanical properties of 5356 aluminum alloy thin walled parts fabricated by laser induced MIG arc enhancement [J]. Weld. Technol., 2017, 46(5): 47
[9] (孙承帅, 张兆栋, 刘黎明. 激光诱导MIG电弧增材制造5356铝合金薄壁零件组织及力学性能 [J]. 焊接技术, 2017, 46(5): 47)
[10] Li Q, Wang F D, Wang G Q, et al. Wire and arc additive manufacturing of lightweight metal components in aeronautics and astronautics [J]. Aeronaut. Manuf. Technol., 2018, 61(3): 74
[10] (李 权, 王福德, 王国庆等. 航空航天轻质金属材料电弧熔丝增材制造技术 [J]. 航空制造技术, 2018, 61(3): 74)
[11] Li F, Chen S J, Shi J B, et al. Evaluation and optimization of a hybrid manufacturing process combining wire arc additive manufacturing with milling for the fabrication of stiffened panels [J]. Appl. Sci., 2017, 7: 1233
[12] H?nnige J R, Colegrove P A, Ahmad B, et al. Residual stress and texture control in Ti-6Al-4V wire+arc additively manufactured intersections by stress relief and rolling [J]. Mater. Des., 2018, 150: 193
[13] Zhang Y M, Chen Y W, Li P, et al. Weld deposition-based rapid prototyping: A preliminary study [J]. J. Mater. Process. Technol., 2003, 135: 347
[14] Mehnen J, Ding J, Lockett H, et al. Design for wire and arc additive layer manufacture [A]. Global Product Development [C]. Berlin Heidelberg: Springer, 2011: 721
[15] Shen C, Pan Z X, Ma Y, et al. Fabrication of iron-rich Fe-Al intermetallics using the wire-arc additive manufacturing process [J]. Addit. Manuf., 2015, 7: 20
[16] Li F, Chen S J, Shi J B, et al. Thermoelectric cooling-aided bead geometry regulation in wire and arc-based additive manufacturing of thin-walled structures [J]. Appl. Sci., 2018, 8: 207
[17] Xiong J T, Geng H B, Lin X, et al. Research status of wire and arc additive manufacture and its application in aeronautical manufacturing [J]. Aeronaut. Manuf. Technol., 2015, (23-24): 80
[17] (熊江涛, 耿海滨, 林 鑫等. 电弧增材制造研究现状及在航空制造中应用前景 [J]. 航空制造技术, 2015, (23-24): 80)
[18] Ding D H, Shen C, Pan Z X, et al. Towards an automated robotic arc-welding-based additive manufacturing system from CAD to finished part [J]. Comput.-Aided Des., 2016, 73: 66
[19] Geng H B, Li J L, Xiong J T, et al. Geometric limitation and tensile properties of wire and arc additive manufacturing 5A06 aluminum alloy parts [J]. J. Mater. Eng. Perform., 2016, 26: 621
[20] Geng H B, Xiong J T, Huang D, et, al. Research status and trends of wire and arc additive manufacturing technology [J]. Weld. Join., 2015, (11): 17
[20] (耿海滨, 熊江涛, 黄 丹等. 丝材电弧增材制造技术研究现状与趋势 [J]. 焊接, 2015, (11): 17)
[21] Xiong J, Zhang G J, Hu J W, et al. Bead geometry prediction for robotic GMAW-based rapid manufacturing through a neural network and a second-order regression analysis [J]. J. Intell. Manuf., 2014, 25: 157
[22] Chen S J, Zhao Y, Xiao J, et al. Robotic wire-arc additive manufacturing for aluminum components [J]. Weld. Join., 2016, (4): 9
[22] (陈树君, 赵 昀, 肖 珺等. 铝合金电弧熔积成形机器人增材制造系统 [J]. 焊接, 2016, (4): 9)
[23] Cao Y, Zhu S, Liang X B, et al. Overlapping model of beads and curve fitting of bead section for rapid manufacturing by robotic MAG welding process [J]. Robot. Comput. -Integr. Manuf., 2011, 27: 641
[24] Xiong J, Zhang G J, Zhang W H. Forming appearance analysis in multi-layer single-pass GMAW-based additive manufacturing [J]. Int. J. Adv. Manuf. Technol., 2015, 80: 1767
[25] Wu B T, Ding D H, Pan Z X, et al. Effects of heat accumulation on the arc characteristics and metal transfer behavior in wire arc additive manufacturing of Ti6Al4V [J]. J. Mater. Process. Technol., 2017, 250: 304
[26] Wang H J, Jiang W H, Ouyang J H, et al. Rapid prototyping of 4043 Al-alloy parts by VP-GTAW [J]. J. Mater. Process. Technol., 2004, 148: 93
[27] Geng H B, Li J L, Xiong J T, et al. Optimisation of interpass temperature and heat input for wire and arc additive manufacturing 5A06 aluminium alloy [J]. Sci. Technol. Weld. Join., 2016, 22: 472
[28] Xiong J, Yin Z Q, Zhang W H. Closed-loop control of variable layer width for thin-walled parts in wire and arc additive manufacturing [J]. J. Mater. Process. Technol., 2016, 233: 100
[29] Doumanidis C, Kwak Y M. Multivariable adaptive control of the bead profile geometry in gas metal arc welding with thermal scanning [J]. Int. J. Press. Vessels Pip., 2002, 79: 251
[30] Martina F, Mehnen J, Williams S W, et al. Investigation of the benefits of plasma deposition for the additive layer manufacture of Ti-6Al-4V [J]. J. Mater. Process. Technol., 2012, 212: 1377
[31] Zhang Y M, Jiang M, Lu W. Double electrodes improve GMAW heat input control [J]. Weld. J., 2004, 83: 39
[32] Zhang R Y, Jiang F, Chen S J, et al. Influence of bypass power mode on electrical properties and droplet transition of arcing-wire PAW [J]. Trans. China Weld. Inst., 2017, 38(2): 41
[32] (张瑞英, 蒋 凡, 陈树君等. 旁路电源工作模式对Arcing-wire PAW电特性与熔滴过渡的影响 [J]. 焊接学报, 2017, 38(2): 41)
[33] Geng Z, Wei Z J, Han X F, et al. Tri-arc double wire arc welding method with high deposition rate and low heat input [J]. MW Met. Form., 2014, (22): 36
[33] (耿 正, 魏占静, 韩雪飞等. 高熔敷率低热输入的Tri-Arc双丝电弧焊接方法 [J]. 金属加工(热加工), 2014, (22): 36)
[34] Chen S J, Zhang L, Wang X P, et al. Stability of the cross-arc process—A preliminary study [J]. Weld. J., 2015, 94: 158
[35] Yang D Q, He C J, Zhang G J. Forming characteristics of thin-wall steel parts by double electrode GMAW based additive manufacturing [J]. J. Mater. Process. Technol., 2016, 227: 153
[36] Huang J K, Yang M H, Li T, et al. Additive manufacturing by double electrode micro-plasma arc welding [J]. J. Shanghai Jiaotong Univ., 2016, 50: 1906
[36] (黄健康, 杨茂鸿, 李 挺等. 旁路耦合微束等离子弧增材制造 [J]. 上海交通大学学报, 2016, 50: 1906)
[37] Song Y A, Park S, Choi D, et al. 3D welding and milling: Part I—A direct approach for freeform fabrication of metallic prototypes [J]. Int. J. Mach. Tools Manuf., 2005, 45: 1057
[38] Jeng J Y, Lin M C. Mold fabrication and modification using hybrid processes of selective laser cladding and milling [J]. J. Mater. Process. Technol., 2001, 110: 98
[39] Xiong X H, Zhang H O, Wang G L, et al. Hybrid plasma deposition and milling for an aeroengine double helix integral impeller made of superalloy [J]. Robot. Comput.-Integr. Manuf., 2010, 26: 291
[40] H?nnige J R, Colegrove P A, Ganguly S, et al. Control of residual stress and distortion in aluminium wire + arc additive manufacture with rolling [J]. Addit. Manuf., 2018, 22: 775
[41] Sun R J, Li L H, Zhu Y, et al. Microstructure, residual stress and tensile properties control of wire-arc additive manufactured 2319 aluminum alloy with laser shock peening [J]. J. Alloys Compd., 2018, 747: 255
[42] Zhu Z C, Dhokia V, Newman S T. The development of a novel process planning algorithm for an unconstrained hybrid manufacturing process [J]. J. Manuf. Process., 2013, 15: 404
[43] Zhu Z C, Dhokia V, Nassehi A, et al. Investigation of part distortions as a result of hybrid manufacturing [J]. Robot. Comput. -Integr. Manuf., 2016, 37: 23
[44] Foroozmehr E, Kovacevic R. Effect of path planning on the laser powder deposition process: Thermal and structural evaluation [J]. Int. J. Adv. Manuf. Technol., 2010, 51: 659
[45] Denlinger E R, Michaleris P. Mitigation of distortion in large additive manufacturing parts [J]. Proc. Inst. Mech. Eng., 2015, 231B: 983
[46] Ding J, Colegrove P, Mehnen J, et al. Thermo-mechanical analysis of wire and arc additive layer manufacturing process on large multi-layer parts [J]. Comput. Mater. Sci., 2011, 50: 3315
[47] Zhou X M, Zhang H O, Wang G L, et al. Three-dimensional numerical simulation of arc and metal transport in arc welding based additive manufacturing [J]. Int. J. Heat Mass Transfer, 2016, 103: 521
[48] Kim T J, Jang B S, Kang S W. Welding deformation analysis based on improved equivalent strain method considering the effect of temperature gradients [J]. Int. J. Naval Archit. Ocean Eng., 2015, 7: 157
[49] Li H. Prediction of welding deformations of ship structures based on inherent strain [D]. Harbin: Harbin Engineering University, 2006
[49] (李 鸿. 基于固有应变的船体分段焊接变形预测 [D]. 哈尔滨: 哈尔滨工程大学, 2006)
[50] Huang X M, Sun J, Li J F. Effect of initial residual stress and machining-induced residual stress on the deformation of aluminium alloy plate [J]. Strojniski Vestnik-J. Mech. Eng., 2015, 61: 131
[51] Sun J, Ke Y L. Study on machining distortion of unitization airframe due to residual stress [J]. Chin. J. Mech. Eng., 2005, 41(2): 117
[51] (孙 杰, 柯映林. 残余应力对航空整体结构件加工变形的影响分析 [J]. 机械工程学报, 2005, 41(2): 117)
[52] Liu M, Takagi J I, Tsukuda A. Effect of tool nose radius and tool wear on residual stress distribution in hard turning of bearing steel [J]. J. Mater. Process. Technol., 2004, 150: 234
[53] Coto B, Navas V G, Gonzalo O, et al. Influences of turning parameters in surface residual stresses in AISI 4340 steel [J]. Int. J. Adv. Manuf. Technol., 2011, 53: 911
[54] Umbrello D, Ambrogio G, Filice L, et al. A hybrid finite element method—Artificial neural network approach for predicting residual stresses and the optimal cutting conditions during hard turning of AISI 52100 bearing steel [J]. Mater. Des., 2008, 29: 873
[55] Salonitis K, D'Alvise L, Schoinochoritis B, et al. Additive manufacturing and post-processing simulation: laser cladding followed by high speed machining [J]. Int. J. Adv. Manuf. Technol., 2016, 85: 2401
[56] Wang S H. Study on initial residual stresses and their effects on milling distortion for thick aero-aluminum-alloy plate [D]. Nanjing: Nanjing University of Aeronautics and Astronautics, 2005
[56] (王树宏. 航空铝合金厚板初始残余应力及其对铣削变形影响的基础研究 [D]. 南京: 南京航空航天大学, 2005)
[57] Wang Q C, Ke Y L. Control and relief of residual stresses in high-strength aluminum alloy parts for aerospace industry [J]. J. Aeronaut. Mater., 2002, 22(3): 59
[57] (王秋成, 柯映林. 航空高强度铝合金残余应力的抑制与消除 [J]. 航空材料学报, 2002, 22(3): 59)
[58] Qi D J. Study on temperature field and stress field of the fused deposition molding process [D]. Kunming: Kunming University of Science and Technology, 2017
[58] (祁冬杰. 熔融沉积成型过程温度场和应力场研究 [D]. 昆明: 昆明理工大学, 2017)
[59] Aggarangsi P, Beuth J. Localized preheating approaches for reducing residual stress in additive manufacturing [A]. Proceedings of SFF symposium [C]. Austin, TX: The University of Texas at Austin, 2006: 709
[60] Colegrove P A, Coules H E, Fairman J, et al. Microstructure and residual stress improvement in wire and arc additively manufactured parts through high-pressure rolling [J]. J. Mater. Process. Technol., 2013, 213: 1782
[61] Vastola G, Zhang G, Pei Q X, et al. Controlling of residual stress in additive manufacturing of Ti6Al4V by finite element modeling [J]. Addit. Manuf., 2016, 12: 231
[62] Bai X W, Zhang H O, Wang G L. Modeling of the moving induction heating used as secondary heat source in weld-based additive manufacturing [J]. Int. J. Adv. Manuf. Technol., 2015, 77: 717
[63] Mohammadi H, Patten J A. Effect of thermal softening on anisotropy and ductile mode cutting of sapphire using micro-laser assisted machining [J]. J. Micro Nano-Manuf., 2017, 5: 011007
[64] Ravindra D, Ghantasala M K, Patten J. Ductile mode material removal and high-pressure phase transformation in silicon during micro-laser assisted machining [J]. Precis. Eng., 36: 364
[65] Ma J F, Pelate N, Lei S T. 3D numerical investigation of thermally assisted high efficiency ductile machining of nanocrystalline hydroxyapatite [J]. J. Manuf. Processes, 2013, 15: 586
[66] Kizaki T, Sugita N, Mitsuishi M. Experimental analysis of the machinability in the thermally assisted milling process of zirconia ceramics [J]. Precis. Eng., 2016, 45: 176
[67] Kim T W, Lee C M. A study on the development of milling process for silicon nitride using ball end-mill tools by laser-assisted machining [J]. Int. J. Adv. Manuf. Technol., 2015, 77: 1205
[68] Tadavani S A, Razavi R S, Vafaei R. Pulsed laser-assisted machining of inconel 718 superalloy [J]. Opt. Laser Technol., 2017, 87: 72
[69] Venkatesan K. The study on force, surface integrity, tool life and chip on laser assisted machining of inconel 718 using Nd: YAG laser source [J]. J. Adv. Res., 2017, 8: 407
[70] Kim D H, Lee C M. A study of cutting force and preheating-temperature prediction for laser-assisted milling of Inconel 718 and AISI 1045 steel [J]. Int. J. Heat Mass Transfer, 2014, 71: 264
[71] Lee I, Bajpai V, Moon S, et al. Tool life improvement in cryogenic cooled milling of the preheated Ti-6Al-4V [J]. Int. J. Adv. Manuf. Technol., 2015, 79: 665
[72] Xi Y, Bermingham M, Wang G, et al. SPH/FE modeling of cutting force and chip formation during thermally assisted machining of Ti6Al4V alloy [J]. Comput. Mater. Sci., 2014, 84: 188
[73] Boschetto A, Bottini L, Veniali F. Finishing of fused deposition modeling parts by CNC machining [J]. Robot. Comput.-Integr. Manuf., 2016, 41: 92
[74] Zhong W W. Experimental research on dry cutting/a little quantity lubricant cutting of aluminum alloy and process fuzzy monitoring [D]. Nanjing: Nanjing University of Aeronautics and Astronautics, 2012
[74] (仲为武. 铝合金干切削和少量润滑切削试验及模糊监控研究 [D]. 南京: 南京航空航天大学, 2012)
[75] Régnier T, Fromentin G, Marcon B, et al. Fundamental study of exit burr formation mechanisms during orthogonal cutting of AlSi aluminium alloy [J]. J. Mater. Process. Technol., 2018, 257: 112
[1] 马健凯, 李俊杰, 王志军, 王俞鉴, 王锦程. 锻造-增材复合制造Ti-6Al-4V合金结合区显微组织及力学性能[J]. 金属学报, 2021, 57(10): 1246-1257.