| 电化学脱合金制备纳米多孔Ag及其甲醛检测性能 |
杨玉林1,穆张岩1,范铮1,淡振华1,2( ),王莹2,常辉1 |
1. 南京工业大学材料科学与工程学院 南京 210009 2. 鞍山钢铁集团公司海洋装备用金属材料及其应用国家重点实验室 鞍山 114021 |
|
| Nanoporous Silver via Electrochemical Dealloying and Its Superior Detection Sensitivity to Formaldehyde |
YANG Yulin1,MU Zhangyan1,FAN Zheng1,DAN Zhenhua1,2( ),WANG Ying2,CHANG Hui1 |
1. College of Materials Science and Engineering, Nanjing Tech University, Nanjing 210009, China 2. State Key Laboratory of Metal Material for Marine Equipment and Application, Anshan Iron and Steel Group Corporation, Anshan 114021, China |
引用本文:
杨玉林, 穆张岩, 范铮, 淡振华, 王莹, 常辉. 电化学脱合金制备纳米多孔Ag及其甲醛检测性能[J]. 金属学报, 2019, 55(10): 1302-1310.
Yulin YANG,
Zhangyan MU,
Zheng FAN,
Zhenhua DAN,
Ying WANG,
Hui CHANG.
Nanoporous Silver via Electrochemical Dealloying and Its Superior Detection Sensitivity to Formaldehyde[J]. Acta Metall Sin, 2019, 55(10): 1302-1310.
| [1] | Xu C X, Xu X H, Su J X ,et al. Research on unsupported nanoporous gold catalyst for CO oxidation [J]. J. Catal., 2007, 252: 243 | | [2] | Zeis R, Lei T, Sieradzki K, et al. Catalytic reduction of oxygen and hydrogen peroxide by nanoporous gold [J]. J. Catal., 2008, 253: 132 | | [3] | Jin Y, Li R, Zhang T. Formation of nanoporous silver by dealloying Ca-Ag metallic glasses in water [J]. Intermetallics, 2015, 67: 166 | | [4] | Qiu H J, Xue L Y, Ji G L, et al. Enzyme-modified nanoporous gold-based electrochemical biosensors [J]. Biosens. Bioelectron., 2009, 24: 3014 | | [5] | Chen Y. The preparation and electrocatalytic properties of nanoporous silver [D]. Guilin: Guangxi Normal University, 2012 | | [5] | (陈 颖. 纳米多孔银的制备及电催化性能研究 [D]. 桂林: 广西师范大学, 2012) | | [6] | Li R, Liu X J, Wang H ,et al. Development of electrochemical supercapacitors with uniform nanoporous silver network [J]. Electrochim. Acta, 2015, 182: 224 | | [7] | Dan Z H, Qin F X, Sugawara Y, et al. Fabrication of nanoporous copper by dealloying amorphous binary Ti-Cu alloys in hydrofluoric acid solutions [J]. Intermetallics, 2012, 29: 14 | | [8] | Dan Z H, Qin F X, Yamaura S I ,et al. Refinement of nanoporous copper by dealloying MgCuY amorphous alloys in sulfuric acids containing polyvinylpyrrolidone [J].J. Electrochem. Soc., 2014, 161: C120 | | [9] | Qin F X, Dan Z H, Hara N ,et al. Selective dissolution of an amorphous Mg65Cu25Y10 alloy in organic acids and dilute HCl solution [J]. Mater. Chem. Phys., 2016, 179: 27 | | [10] | Dan Z H, Qin F X, Wada T, et al. Nanoporous palladium fabricated from an amorphous Pd42.5Cu30Ni7.5P20 precursor and its ethanol electro-oxidation performance [J]. Electrochim. Acta, 2013, 108: 512 | | [11] | Zhang C, Sun J Z, Xu J L ,et al. Formation and microstructure of nanoporous silver by dealloying rapidly solidified Zn-Ag alloys [J]. Electrochim. Acta, 2012, 63: 302 | | [12] | Forty A J, Durkin P. A micromorphological study of the dissolution of silver-gold alloys in nitric acid [J]. Philos. Mag., 1980, 42A: 295 | | [13] | Erlebacher J, Aziz M J, Karma A ,et al. Evolution of nanoporosity in dealloying [J]. Nature, 2001, 410: 450 | | [14] | Song T T, Gao Y L, Zhang Z H ,et al. Influence of magnetic field on dealloying of Al-25Ag alloy and formation of nanoporous Ag [J]. CrystEngComm, 2012, 14: 3694 | | [15] | Ji H, Wang X G, Zhao C C ,et al. Formation, control and functionalization of nanoporous silver through changing dealloying media and elemental doping [J]. CrystEngComm, 2011, 13: 2617 | | [16] | Zhang M, Junior A M J, Pang S J, et al. Fabrication of nanoporous silver with open pores [J]. Scr. Mater., 2015, 100: 21 | | [17] | Li Z Q, Wang X M, Lu X. Refinement of nanoporous silver by adding surfactant to the electrolyte [J]. ECS Electrochem. Lett., 2014, 3: C13 | | [18] | Cui Y L. Improving of the method of formaldehyde manual titration [J]. Chem. Eng. Des. Commun., 2014, 40(3): 51 | | [18] | (崔永乐. 手动滴定测定甲醛方法的改进 [J]. 化学设计通讯, 2014, 40(3): 51) | | [19] | Yao J D, Sun D, Zhong C H, et al. Determination of formaldehyde content in soil by acetylacetone spectrophotometry [J]. Chem. Anal. Meterage, 2017, 26(1): 85 | | [19] | (姚洁丹, 孙 丹, 钟灿红等. 乙酰丙酮分光光度法测定土壤中甲醛 [J]. 化学分析计量, 2017, 26(1): 85) | | [20] | Gao M H, Zhou S L, Yang Z Y ,et al. Spectrophotometric determination of formaldehyde in water sample with amino acid-acetylacetone [J]. Phys. Test. Chem. Anal., 2014, 50B: 50 | | [20] | (高明慧, 周仕林, 杨卓圆等. 氨基酸-乙酰丙酮分光光度法测定水样中甲醛 [J]. 理化检验, 2014, 50B: 50) | | [21] | Dai Z R, Lin M F, Zhang C X. Rapid detection of formaldehyde content in fresh milk by gas chromatography [J]. Food Res. Dev., 2015, 36(24): 154 | | [21] | (戴梓茹, 林美芳, 张晨晓. 气相色谱法快速测定鲜牛乳中的甲醛含量 [J]. 食品研究与开发, 2015, 36(24): 154) | | [22] | Xu J L, Wang Y, Zhang Z H. Potential and concentration dependent electrochemical dealloying of Al2Au in sodium chloride solutions [J]. J. Phys. Chem., 2012, 116C: 5689 | | [23] | Zhang Q, Wang X G, Qi Z ,et al. A benign route to fabricate nanoporous gold through electrochemical dealloying of Al-Au alloys in a neutral solution [J]. Electrochim. Acta, 2009, 54: 6190 | | [24] | Fu C Q, Xu L J, Dan Z H, et al. Annealing effect of amorphous Fe-Si-B-P-Cu precursors on microstructural evolution and redox behavior of nanoporous counterparts [J]. J. Alloys Compd., 2017, 726: 810 | | [25] | Zhang Q, Zhang Z H. On the electrochemical dealloying of Al-based alloys in a NaCl aqueous solution [J]. Phys. Chem. Chem. Phys., 2010, 12: 1453 | | [26] | Dursun A, Pugh D V, Corcoran S G. Dealloying of Ag-Au alloys in halide-containing electrolytes: Affect on critical potential and pore size [J]. J. Electrochem. Soc., 2003, 150: B355 | | [27] | Yang C L, Xiang Y, Yang S C ,et al. Nanoporous gold by dealloying and its electrocatalytic oxidation abilities towards glucose [J]. Rare Met. Mater. Eng., 2014, 43: 230 | | [27] | (杨春雷, 项 桦, 杨圣晨等. 纳米多孔金的制备及其对葡萄糖催化性能研究 [J]. 稀有金属材料与工程, 2014, 43: 230) | | [28] | Sun Y, Ye J, Shan Z W ,et al. The mechanical behavior of nanoporous gold thin films [J]. JOM, 2007, 59(9): 54. | | [29] | Bai L. Study on the electrocatalysis properties of nanoporous silver [D]. Dalian: Dalian Jiaotong University, 2015 | | [29] | (白 璐. 多孔银的电催化性能研究[D]. 大连: 大连交通大学, 2015) | | [30] | Zhao Y, Qin S J, Li Y ,et al. Electrodeposition of dendritic Pd nanoarchitectures on n-GaN(0001): Nucleation and electrocatalysis for direct formic acid fuel cells [J]. Electrochim. Acta, 2014, 145: 148 | | [31] | Duan D H, Liu H H, You X, et al. Anodic behavior of carbon supported Cu@Ag core-shell nanocatalysts in direct borohydride fuel cells [J]. J. Power Sources, 2015, 293: 292 | | [32] | Yu Y N, Jia M Z, Tian H F ,et al. The fabrication of silver ion implantation-modified electrode and its application in electrocatalytic oxidation of formaldehyde [J]. J. Power Sources, 2014, 267: 123 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|