| 熔池三维自由表面状态与TIG焊熔透的相关性研究* |
张刚, 石玗( ), 李春凯, 黄健康, 樊丁 |
| 兰州理工大学省部共建有色金属先进加工与再利用国家重点实验室, 兰州 730050 |
|
| RESEARCH ON THE CORRELATION BETWEEN THE STATUS OF THREE-DIMENSIONAL WELD POOL SURFACE AND WELD PENETRATION IN TIG WELDING |
ZHANG Gang, SHI Yu( ), LI Chunkai, HUANG Jiankang, FAN Ding |
| State Key Laboratory of Advanced Processing and Recycling of Nonferrous Metals, Lanzhou University of Technology, Lanzhou 730050 |
引用本文:
张刚, 石玗, 李春凯, 黄健康, 樊丁. 熔池三维自由表面状态与TIG焊熔透的相关性研究*[J]. 金属学报, 2014, 50(8): 995-1002.
Gang ZHANG,
Yu SHI,
Chunkai LI,
Jiankang HUANG,
Ding FAN.
RESEARCH ON THE CORRELATION BETWEEN THE STATUS OF THREE-DIMENSIONAL WELD POOL SURFACE AND WELD PENETRATION IN TIG WELDING[J]. Acta Metall Sin, 2014, 50(8): 995-1002.
| [1] |
Liu L M, Zhang Z D, Shen Y, Wang L. Acta Metall Sin, 2006; 42: 399
|
| [1] |
(刘黎明, 张兆栋, 沈 勇, 王 来. 金属学报, 2006; 42: 399)
|
| [2] |
Mills K C, Keene B J. Int Mater Rev, 1990; 35: 185
|
| [3] |
Lucas W, Bertaso D, Melton G, Smith J, Balfour C. Weld Int, 2012; 4: 243
|
| [4] |
Pal K, Pal S K. Mater Manuf Process, 2011; 26: 684
|
| [5] |
Chokkalingham S, Chandrasekhar N, Vasudevan M. J Intell Manuf, 2012; 23: 1995
|
| [6] |
Richardson R W, Gutow D A, Anderson R A, Farson D F. Weld J, 1984; 63: 43
|
| [7] |
Bae K Y, Lee T H, Ahn K C. J Mater Process Technol, 2002; 120: 458
|
| [8] |
Zhao D B, Chen Q, Chen S B, Wu L. Opt Technol, 2001; 27: 367
|
| [8] |
(赵冬斌, 陈 强, 陈善本, 吴 林. 光学技术, 2001; 27: 367)
|
| [9] |
Li L P, Lin T, Chen S B, Yang X Q. J Shanghai Jiaotong Univ, 2006; 40: 898
|
| [9] |
(李来平, 林 涛, 陈善本, 杨学勤. 上海交通大学学报, 2006; 40: 898)
|
| [10] |
Mnich C, Al-Bayat F, Debrunner C, Steele J, Vincent T. Proc 2004 Japan-USA Symposium on Flexible Automation, Denver, CO, 2004: 19
|
| [11] |
Kovacevic R, Zhang Y M. J Manuf Sci Eng, 1997; 119: 161
|
| [12] |
Kovacevic R, Zhang Y M, Ruan S. J Eng Ind, 1995; 117: 210
|
| [13] |
Liu M Y. Master Thesis, Harbin Institute of Technology, 2007
|
| [13] |
(刘鸣宇. 哈尔滨工业大学硕士学位论文, 2007)
|
| [14] |
Ai X P, Liu N S, Wei Y Q, Hu X. Trans China Weld Inst, 2011; 32(3): 85
|
| [14] |
(艾孝谱, 刘南生, 魏义庆, 胡 仙. 焊接学报, 2011; 32(3): 85)
|
| [15] |
Saeed G, Zhang Y M. Meas Sci Technol, 2003; 14: 1671
|
| [16] |
Song H S, Zhang Y M. Meas Sci Technol, 2007; 18: 3751
|
| [17] |
Song H S, Zhang Y M. Weld J, 2008; 87: 85-s
|
| [18] |
Xiao Y H, Denouden G. Weld J, 1993; 72: 428-s
|
| [19] |
Shi Y, Zhang G, Ma X J, Fan D. Chin J Mech Eng, 2012; 48(24): 28
|
| [19] |
(石 玗, 张 刚, 马小骥, 樊 丁. 机械工程学报, 2012; 48(24): 28)
|
| [20] |
Wu C S, Zhao P C. Acta Metall Sin, 2006; 42: 865
|
| [20] |
(武传松, 赵朋成. 金属学报, 2006; 42: 865)
|
| [21] |
Zhao M, Wu C S, Chen J. Chin J Mech Eng, 2007; 43(6): 68
|
| [21] |
(赵 明, 武传松, 陈 姬. 机械工程学报, 2007; 43(6): 68)
|
| [22] |
He J S, Yang C L, Lin S B, Wang Q L. Mater Sci Technol, 2001; 9(1): 26
|
| [22] |
(何景山, 杨春利, 林三宝, 王其隆. 材料科学与工艺, 2001; 9(1): 26)
|
| [23] |
Rokhlin S I, Guu A C. Weld J, 1993; 72: 381-s
|
| [24] |
Wang Z Z, Zhang Y M, Yang R G. J Manuf Process, 2013; 15: 34
|
| [25] |
Liu Y K, Zhang W J, Zhang Y M. Weld J, 2013; 92: 313-s
|
| [26] |
Ma H B, Wei S C. Sensor Rev, 2010; 30: 116
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|