Au反点阵列孔径对Au/TiO2复合薄膜光催化性能的影响 |
祁洪飞1( ), 刘大博1, 滕乐金1, 王天民2, 罗飞1, 田野1 |
1 中航工业北京航空材料研究院钢与稀贵金属研究所, 北京 100095 2 北京航空航天大学凝聚态物理与材料物理研究中心, 北京 100191 |
|
EFFECT OF PORE SIZES OF Au ANTIDOT ARRAYS ON PHOTOCATALYSIS PERFORMANCE OF Au/TiO2 COMPOSITE FILMS |
QI Hongfei1( ), LIU Dabo1, TENG Lejin1, WANG Tianmin2, LUO Fei1, TIAN Ye1 |
1 Department of Steel and Rare-Noble Metals, AVIC Beijing Institute of Aeronautical Materials, Beijing 100095 2 Center of Condensed Matter and Material Physics, Beihang University, Beijing 100191 |
引用本文:
祁洪飞, 刘大博, 滕乐金, 王天民, 罗飞, 田野. Au反点阵列孔径对Au/TiO2复合薄膜光催化性能的影响[J]. 金属学报, 2014, 50(10): 1163-1169.
Hongfei QI,
Dabo LIU,
Lejin TENG,
Tianmin WANG,
Fei LUO,
Ye TIAN.
EFFECT OF PORE SIZES OF Au ANTIDOT ARRAYS ON PHOTOCATALYSIS PERFORMANCE OF Au/TiO2 COMPOSITE FILMS[J]. Acta Metall Sin, 2014, 50(10): 1163-1169.
[1] |
Chen X, Liu L, Yu P Y, Mao S S. Science, 2011; 331: 746
|
[2] |
Wang H Q, Shen H, Ba D C, Wang B W, Wen L S, Chen D. Acta Metall Sin (Engl Lett), 2005; 18: 194
|
[3] |
Niibe M, Sano K, Kotaka T, Kawakami R, TominAua K, Nakano Y. J Appl Phys, 2013; 113: 126101
|
[4] |
Li Z G, Miyake S. Acta Metall Sin, 2010; 46: 13
|
[4] |
(李铸国, 三宅正司. 金属学报, 2010; 46: 13)
|
[5] |
Zhang M, Lin G Q, Dong C, Wen L S. Acta Metall Sin, 2007; 43: 509
|
[5] |
(张 敏, 林国强, 董 闯, 闻立时. 金属学报, 2007; 43: 509)
|
[6] |
Wang T M, Wang Y. Mater China, 2010; 29: 60
|
[6] |
(王天民, 王 莹. 中国材料进展, 2010; 29: 60)
|
[7] |
Zhang Y G, Wang Y X. J Appl Phys, 2011; 110: 033519
|
[8] |
Zeng Y, Liu J T, Qian W J, Gao J H. Acta Metall Sin (Engl Lett), 2005; 18: 363
|
[9] |
Wang Y, Zhao D, Ji H, Liu G, Chen C, Ma W, Zhu H, Zhao J. J Phys Chem, 2010; 114C: 17728
|
[10] |
Pandikumar A, Murugesan S, Ramaraj R. Appl Mater Interf, 2010; 2: 1912
|
[11] |
Zhang Y, Wang Q, Xu J, Ma S. Appl Surf Sci, 2012; 258: 10104
|
[12] |
Chiarello G L, Ferri D, Selli E. J Catal , 2011; 280: 168
|
[13] |
Lucjan C, Maudalena J, Adam S, Zofia P, Aunieszka W, Stefan W, Marek M. Appl Catal, 2013; 130B: 152
|
[14] |
Stepanov A L. Rev Adv Mater Sci, 2012; 30: 150
|
[15] |
Adochite R C, Munteanu D, Torrell M, Cunha L, Alves E, Barradas N P, Cavaleiro A, Riviere J P, Le Bourhis E, Eyidi D, Vaz F. Appl Surf Sci, 2012; 258: 4028
|
[16] |
Chakravadhanula V S K, Hrkac T, Zaporojtchenko V, Podschun R, Kotnur V G, Kulkarni A, Strunskus T, Kienle L, Faupel F. J Nanosci Nanotechno, 2011; 11: 4893
|
[17] |
Wang C, Yin L, Zhang L, Liu N, Lun N, Qi Y. Appl Mater Interf, 2010; 2: 3373
|
[18] |
Zhang X, Meng H, Sun T, Zhou C B. Acta Metall Sin, 2008; 44: 1394
|
[18] |
(张 霞, 孟 皓, 孙 挺, 周春彬. 金属学报, 2008; 44: 1394)
|
[19] |
Lazau C, Ratiu C, Orha C, Pode R, Manea F. Mater Res Bull, 2011; 46: 1916
|
[20] |
Qi H F, Hao W C, Xu H Z, Zhang J Y, Wang T M. Colloid Polym Sci, 2009; 287: 243
|
[21] |
Minchitha K U, Geetha Balakrishna R. Mater Chem Phys, 2012; 136: 720
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|