| 行波磁场下吹Ar过程中结晶器内气泡行为的研究 |
| 陈芝会,王恩刚,张兴武,王元华,朱明伟,赫冀成 |
| 东北大学材料电磁过程研究教育部重点实验室, 沈阳 110819 |
|
| STUDY ON THE BEHAVIOUR OF BUBBLES IN A CONTINUOUS CASTING MOLD WITH Ar INJECTION AND TRAVELING MAGNETIC FIELD |
| CHEN Zhihui, WANG Engang, ZHANG Xingwu,WANG Yuanhua, ZHU Mingwei, HE Jicheng |
| Key Laboratory National Education Ministry for Electromagnetic Processing of Materials, Northeastern University, Shenyang 110819 |
引用本文:
陈芝会 王恩刚 张兴武 王元华 朱明伟 赫冀成. 行波磁场下吹Ar过程中结晶器内气泡行为的研究[J]. 金属学报, 2012, 48(8): 951-956.
,
,
,
,
,
.
STUDY ON THE BEHAVIOUR OF BUBBLES IN A CONTINUOUS CASTING MOLD WITH Ar INJECTION AND TRAVELING MAGNETIC FIELD[J]. Acta Metall Sin, 2012, 48(8): 951-956.
| [1] Thomas B G, Zhang L. ISIJ Int, 2001; 41: 1181[2] Zhang L F, Yang S B, Cai K K, Li J Y, Wan X G, Thomas B G. Metall Mater Trans, 2007; 38B: 63[3] Singh V, Dash S K, Sunitha J S, Ajmani S K, Das A K. ISIJ Int, 2006; 46: 210[4] Cukierski K, Thomas B G. Metall Mater Trans, 2008; 39B: 94[5] Garcia–Hernandez S, Morales R D, Torres–Alonso E. Ironmaking Steelmaking, 2010; 37: 360[6] Timmel K, Eckert S, Gerbeth G. Metall Mater Trans, 2011; 42B: 68[7] Yu H Q, Zu M Y. ISIJ Int, 2008; 48: 584[8] Kunstreich S, Dauby P H. Ironmaking Steelmaking, 2005; 32: 80[9] Kubo N, Kubota J, Suzuki M, Ishii T. ISIJ Int, 2007; 47: 988[10] Miki Y, Takeuchi S. ISIJ Int, 2003; 43: 1548[11] Kwon Y, Zhang J, Lee H G. ISIJ Int, 2006; 46: 257[12] Yamashita S, Iguchi M. ISIJ Int, 2001; 41: 1529[13] Takatani K, Tanizawa Y, Mizukami H, Nishimura K. ISIJ Int, 2001; 41: 1252[14] Zhang S J, Zhu M Y, Zhang Y L, Zheng S G, Cheng N L, Song J X. Acta Metall Sin, 2006; 42: 1087(张胜军, 朱苗勇, 张永亮, 郑书国, 程乃良, 宋景欣. 金属学报, 2006; 42: 1087)[15] Cao N, Zhu M Y. Acta Metall Sin, 2008; 44: 79(曹娜, 朱苗勇. 金属学报, 2008; 44: 79)[16] Wang Y F, Dong A P, Zhang L F. Steel Res Int, 2011; 82: 428[17] Lei Z S, Zhang H B, Ren Z M, Deng K, Zhong Y B. 6th Int Conf on Electromagnetic Processing of Materials, Dresden, Germany: Forschungszentrum Dresden–Rossendrof, 2009: 575[18] Yu H Q, Zhu M Y. Acta Metall Sin, 2008; 44: 619(于海岐, 朱苗勇. 金属学报, 2008; 44: 619)[19] Yavuz M M. Steel Res Int, 2011; 82: 809[20] Yu Z, Zhang Z Q, Ren Z M, Lei Z S, Deng K. Acta Metall Sin, 2010; 46: 1275(于湛, 张振强, 任忠鸣, 雷作胜, 邓康. 金属学报, 2010; 46: 1275)[21] Kubo N, Ishii T, Kubota J, Ikagawa T. ISIJ Int, 2004; 44: 556[22] Kubota J, Kubo N, Ishii T, Suzuki M, Aramaki N, Nishimachi R. NKK Technol Rev, 2001; 85: 1[23] Toh H, Hasegawa H, Harada H. ISIJ Int, 2001; 41: 1245[24] Wang X D, Fautrelle Y, Etay J, Moreau R. Metall Mater Trans, 2009; 40B: 82[25] Wang H D, Zhu M Y, Yu H Q. J Iron Steel Res Int, 2010; 17: 25[26] Wang T F, Wang J F, Yang W G, Jin Y. J Chem Eng, 2001; 52: 197(王铁峰, 王金福, 杨卫国, 金涌. 化工学报, 2001; 52: 197) |
|