					引用本文:
						|  |  
    					|  |  
    					| (Ti, Al)N涂层应力沿层深分布的调整及大厚度涂层的制备 |  
						| 赵升升1), 程毓1), 常正凯2), 王铁钢2), 孙超2) |  
					| 1) 深圳职业技术学院, 深圳 518055 2) 中国科学院金属研究所, 沈阳 110016
 |  
						|  |  
    					| MODIFICATION OF STRESS DISTRIBUTION ALONG THE THICKNESS OF (Ti, Al)N COATINGS AND PREPARATION OF THE COATINGS WITH LARGE THICKNESS |  
						| ZHAO Shengsheng1), CHENG Yu1), CHANG Zhengkai2), WANG Tiegang2), SUN Chao2) |  
						| 1) Shenzhen Polytechnic, Shenzhen 518055 2) Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
 |  
								赵升升 程毓 常正凯 王铁钢 孙超. (Ti, Al)N涂层应力沿层深分布的调整及大厚度涂层的制备[J]. 金属学报, 2012, 48(3): 277-282.	
																												,
																								 ,
																								 ,
																								 ,
																												 . 
				MODIFICATION OF STRESS DISTRIBUTION ALONG THE THICKNESS OF (Ti, Al)N COATINGS AND PREPARATION OF THE COATINGS WITH LARGE THICKNESS[J]. Acta Metall Sin, 2012, 48(3): 277-282.
 
					
						| 
								
									|  
          
          
            
                         
            
									            
									                
																														  
																| [1] Palmers J, Van Stappen M. Surf Coat Technol, 1995; 76/77: 363[2] Shew B Y, Huang J L. Surf Coat Technol, 1995; 71: 30[3] Cheng Y H, Tay B K, Lau S P, Shi X, Chua H C. Thin Solid Films, 2000; 379: 76[4] Zhao S S, Yang Y, Li J B, Gong J, Sun C. Surf Coat Technol, 2008; 202: 5185[5] Huang J H, Ma C H, Chen H. Surf Coat Technol, 2006; 201: 3199[6] Sun X L, Fan Z X, Shao J D. Acta Metall Sin, 2007; 43: 307(孙喜莲, 范正修, 邵建达. 金属学报, 2007; 43: 307)[7] Song G H, Zheng J D, Liu Y, Sun C. J Synth Crys, 2004; 33: 422[8] Stein C, Keunecke, M, Bewilogua K, Chudoba T, Koelker W, van den Berg H. Surf Coat Technol, 2011; 205(spec): 2[9] Wu P, Zhou C Z, Tang X N. Acta Metall Sin, 1994; 30: 508(吴萍, 周昌炽, 唐西南. 金属学报, 1994; 30: 508)[10] PalDey S, Deevi S C. Mater Sci Eng, 2003; A361: 1[11] Manaila R, Devenyi A, Biro D, David L, Barna P B, Kovacs A. Surf Coat Technol, 2002; 151: 21[12] Li M S, Wang F H. Surf Coat Technol, 2003; 167: 197[13] Sanchette F, Czerwiec T. Surf Coat Technol, 1997; 96: 184[14] Paul H M, Christian M, Lars H, Helmut C. Prog Mater Sci, 2006; 51: 1032[15] Zhao S S, Du H, Hua W G, Gong J, Li J B, Sun C. J Mater Res, 2007; 22: 2659[16] Yang H G, Li S, Zhang R L. China Surf Eng, 2009; 22(2): 20(杨洪刚, 李曙, 张荣禄.中国表面工程, 2009; 22(2): 20)[17] Wang T G, Zhao S S, Hua W G, Li J B, Gong J, Sun C. Mater Sci Eng, 2010; A527: 454[18] Zhou Y, Rao G B, Wang J Q, Zhang B, Yu Z M, Ke W, Han E H. Thin Solid Films, 2011; 519: 2207[19] Wan X S, Zhao S S, Yang Y, Gong J, Sun C. Surf Coat Technol, 2010; 204: 1800[20] Yang Y, Zhao S S, Gong J, Jiang X, Sun C. J Mater Sci Technol, 2011; 27: 385[21] Josson B, Hogmark S. Thin Solid Films, 1984; 114: 257[22] Zheng J D, Zou Y S, Song G H, Gong J, Liu Y, Sun C, Wen L S. Acta Metall Sin, 2004; 40: 745(郑静地, 邹友生, 宋贵宏, 宫骏, 刘 越, 孙超, 闻立时. 金属学报, 2004; 40: 745)[23] Thornton J A. Ann Rev Mater Sci, 1977; 7: 239[24] Tian M B, Liu D L. Film Science and Technology Handbook (1st Vol.). Beijing: China Machine Press, 1980: 7(田民波, 刘德令. 薄膜科学与技术手册 (上). 北京: 机械工业出版社, 1980: 7)[25] Carvalho N J M, Zoestbergen E, Kooi B J, Hosson D J T M. Thin Solid Films, 2003; 429: 179 |  
             
												
											    	