| 加热过程中硫系易切削钢中MnS夹杂物行为的动态原位观察 |
| 邵肖静, 王新华, 姜敏, 王万军, 黄福祥, 冀云卿 |
| 北京科技大学冶金与生态工程学院, 北京 100083 |
|
| IN SITU OBSERVATION OF MnS INCLUSION BEHAVIOR IN RESULFURIZED FREE-CUTTING STEEL DURING HEATING |
| SHAO Xiaojing, WANG Xinhua, JIANG Min, WANG Wanjun, HUANG Fuxiang, JI Yunqing |
| School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
邵肖静 王新华 姜敏 王万军 黄福祥 冀云卿. 加热过程中硫系易切削钢中MnS夹杂物行为的动态原位观察[J]. 金属学报, 2011, 47(9): 1210-1215.
,
,
,
,
,
.
IN SITU OBSERVATION OF MnS INCLUSION BEHAVIOR IN RESULFURIZED FREE-CUTTING STEEL DURING HEATING[J]. Acta Metall Sin, 2011, 47(9): 1210-1215.
| [1] Chen H X, Zhou P, Chen A J, L¨u H L, Li C F. China Metall, 2001; 11: 32(陈洪星, 周平, 陈爱洁, 吕洪亮, 李丰常. 中国冶金, 2001; 11: 32)[2] Jiang G H. Master Dissertation, Kunming University of Science and Technology, 2006(蒋光辉. 昆明理工大学硕士学位论文, 2006)[3] Mao Z Q. Auto Technol Mater, 2000; 2: 1(毛志强. 汽车工艺与材料, 2000; 2: 1)[4] Li Y M, Zhu F X, Cui F P, Fang K. J Northeastern Univ (Nat Sci), 2007; 28: 1002(李艳梅, 朱伏先, 崔凤平, 房 轲. 东北大学学报(自然科学版), 2007; 28: 1002)[5] Chen M, Liu G, Zhang X H, Shen Z, Yang G J. Chin J Mechan Eng, 2007; 43: 161(陈明, 刘钢, 张晓辉, 沈中, 杨贵军. 机械工程学报, 2007; 43: 161)[6] Xu J, Xu D S, Li L C, Xiong L L, Wang J F. Auto Sci Technol, 2003; 1: 28(许俊, 徐德生, 李良策, 熊龙亮, 王劲枫. 汽车科技, 2003; 1: 28)[7] Li L S, Zhu R, Dong J. In: Li W X ed., CSM 2003 Annual Meeting Proceedings, Beijing: Metallurigical Industry Press, 2003: 335(李联生, 朱 荣, 董杰. 见: 李文秀主编, 2003中国钢铁年会论文集, 北京: 冶金工业出版社, 2003: 335)[8] Xia Y J,Wang F M,Wang J L, Zhao J. J Univ Sci Technol Beijing, 2010; 32B: 1271(夏云进, 王福明, 王金龙, 赵晶. 北京科技大学学报, 2010; 32B: 1271)[9] Chen L, Chen W Q, Xiao F H. Spec Steel, 2008; 29: 47(陈列, 陈伟庆, 肖飞虎. 特殊钢, 2008; 29: 47)[10] Li G Z, Wang F M, Hui R, Cao W K. Int J Miner Metall Mater, 2009; 16: 650[11] Li L S, Zhu R, Yin H, Liu P, Zhang L P, Wei C Z, Zhou P, Dong J. Chin Rare Earths, 2005; 26(5): 48(李联生, 朱 荣, 殷浩, 刘平, 张利平, 魏承志, 周平, 董杰. 稀土, 2005; 26(5): 48)[12] Yun G A, Qin Z, Tian Z H, Sun Y H,Cai K K. J Univ Sci Technol Beijing, 2007; 29B: 685(严国安, 秦哲, 田志红, 孙彦辉, 蔡开科. 北京科技大学学报, 2007; 29B: 685)[13] Shao X J, Wang X H, Wang W J, Huang F X, Jiang M. J Univ Sci Technol Beijing, 2010; 32B: 570(邵肖静, 王新华, 王万军, 黄福祥, 姜敏. 北京科技大学学报, 2010; 32B: 570)[14] Nichols F A. J Mater Sci, 1976; 11: 1077[15] Nichols F A, MullinsWW. Trans Metall Soc AIME, 1965; 233: 1840[16] Liu W J, Jonas J J. Metall Trans, 1989; 20A: 1361 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|