| 镍基双晶高温合金定向凝固过程中的竞争生长 |
| 卢琦1,2,李金国3,金涛2,周亦胄2,孙晓峰2,胡壮麒4 |
1.
2. 中国科学院金属研究所
3. 中科院金属研究所
4. 中国科学院金属研究所高温合金部 |
|
| COMPETITIVE GROWTH IN BI-CRYSTAL OF NI-BASED SUPERALLOYS DURING DIRECTIONAL SOLIDIFICATION |
引用本文:
卢琦 李金国 金涛 周亦胄 孙晓峰 胡壮麒. 镍基双晶高温合金定向凝固过程中的竞争生长[J]. 金属学报, 2011, 47(6): 641-648.
| [1] Ross E W, O’Hara K S. Superalloys 1996, edited by Kissinger R D, Deye D J, Cetel A D, Nathal M V, Pollock T M, Woodford D A. Warrendale, PA: TMS, 1996: 19[2] Cetel A D, Duhl D N. Superalloys 1988, edited by Reichman S, Duhl D N, Maurer G, Antolovich S, Lund C. Warrendale, PA: TMS, 1988: 235[3] Li J R, Zhao J Q, Liu S Z, Han M. Superalloys 2008, edited by Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S A. Warrendale, PA: TMS, 2008: 443[4] Gell M, Duhl D, Gupta D K, Sheffler K D. J Metals, 1987; 7: 11[5] Kear B H, Piearcey B J. Trans Metall Soc AIME, 1967; 239: 1209[6] Quested P N, McLean M. Mater Sci Eng, 1984; 65: 171[7] McLean M. Directionally Solidified Materials for High Temperature Service. London: Metals Society, 1983: 5[8] Walton D, Chalmers B. Trans Metall Soc AIME, 1959; 215: 447[9] Zhou Y Z, Volek A, Green N R. Acta Mater, 2008; 56: 2631[10] Ardakani M G, D’Souza N, Wagner A, Shollock B A, McLean M. Superalloy 2000, edited by Pollock T M, Kissinger R D, Bowman R R, Green K A, McLean M, Olson S, Schirra J J. Warrendale, PA: TMS, 2000: 219[11] Wagner A, Shollock B A, McLean M. Mater Sci Eng, 2004; A374: 270[12] Zhou Y Z, Green N R. Superalloy 2008, edited by Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S A. Warrendale, PA: TMS, 2008: 317[13] D’Souza N, Ardakani M G, McLean M, Shollock B A. Metall Mater Trans, 2000; 31A: 2877[14] D’Souza N, Ardakani M G, Wagner A, Shollock B A, McLean M. J Mater Sci, 2002; 37: 481[15] Liu Z Y, Lei Y, Fu H Z. Acta Mater Sin, 2000; 36: 1(刘志义, 雷毅, 傅恒志. 金属学报, 2000; 36: 1)[16] D’Souza N, Jennings P A, Yang X L, Dong H B, McLean M. Metall Mater Trans, 2005; 36B: 657 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|