| 利用电化学方法测定高温银液中氧的扩散系数 |
| 高运明1); 宋建新1); 张业勤1); 郭兴敏2) |
| 1) 武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室; 武汉 430081 2) 北京科技大学冶金与生态工程学院; 北京 100083 |
|
| MEASUREMENT OF THE DIFFUSIVITY OF OXYGEN IN HIGH-TEMPERATURE LIQUID SILVER BY ELECTROCHEMICAL METHOD |
| GAO Yunming1); SONG Jianxin1); ZHANG Yeqin1); GUO Xingmin2) |
| 1) Key Laboratory for Ferrous Metallurgy and Resources Utilization of Ministry of Education; Wuhan University of Science and Technology; Wuhan 430081 2) Metallurgical and Ecological Engineering School; University of Science and Technology Beijing; Beijing 100083 |
引用本文:
高运明 宋建新 张业勤 郭兴敏. 利用电化学方法测定高温银液中氧的扩散系数[J]. 金属学报, 2010, 46(3): 277-281.
,
,
,
.
MEASUREMENT OF THE DIFFUSIVITY OF OXYGEN IN HIGH-TEMPERATURE LIQUID SILVER BY ELECTROCHEMICAL METHOD[J]. Acta Metall Sin, 2010, 46(3): 277-281.
| [1] Chou K C, Gao Y M, Guo X M, Lu X G, Xu K D. Proc 10th Japan–China Symposium on Science and Technology of Iron and Steel. Tokyo: The Iron and Steel Institute of Japan, 2004: 162
[2] Gao Y M, Guo X M, Chou K C. J Chongqing Univ, 2006; 29(8): 123
(高运明, 郭兴敏, 周国治. 重庆大学学报, 2006; 29(8): 123)
[3] Pal Uday B. JOM, 2008; 60: 43
[4] Shah I D, Parlee N A D. Trans TMS–AIME, 1967; 239: 763
[5] Mizikar E A, Grace R E, Parlee N A D. Trans ASM, 1963; 56: 101
[6] Masson C R, Whiteway S G. Can Metall Q, 1967; 6: 199
[7] Sano N, Honma S, Matsushita Y. Metall Trans, 1970; 1: 301
[8] Otsuka S, Kozuka Z. Trans JIM, 1974; 15: 32
[9] Oberg K E, Friedman L M, Boorstein W M, Rapp R A. Metall Trans, 1973; 4: 61
[10] Rickert H, El Miligy A A. Z Metallk, 1968; 59: 635
[11] Otsuka S, Katayama I, Kozuka Z. Trans JIM, 1971; 12: 442
[12] Ramanarayanan T A, Rapp R A. Metall Trans, 1972; 3: 3239
[13] Bernard G, Lupis C H P. Metall Trans, 1971; 2: 555
[14] He C X. Phase Diagrams and Structural Parameter of Alloys and Compound of Noble Metal. Beijing: Metallurgical Industry Press, 2007: 24, 26
(何纯孝. 贵金属合金相图及化合物结构参数.北京: 冶金工业出版社, 2007: 24, 26) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|