| 脉冲电磁场对CoC2O4 ·2H2O粒度的影响 |
| 杜慧玲1;2;王建中2;齐锦刚2;何力佳2;苍大强1 |
1. 北京科技大学冶金与生态工程学院; 北京 100083
2. 辽宁工业大学材料与化学工程学院; 锦州 121001 |
|
| EFFECTS OF PULSED ELECTROMAGNETIC FIELD ON CoC2O4·2H2O POWDER SIZE |
| DU Huiling 1;2; WANG Jianzhong 2; QI Jingang 2; HE Lijia 2; CANG Daqiang 1 |
1. School of Metallurgical and Ecological Engineering; University of Science and Technology Beijing; Beijing 100083
2. School of Material and Chemical Engineering; Liaoning University of Technology; Jinzhou 121001 |
引用本文:
杜慧玲 王建中 齐锦刚 何力佳 苍大强. 脉冲电磁场对CoC2O4 ·2H2O粒度的影响[J]. 金属学报, 2009, 45(8): 1019-1024.
,
,
,
,
.
EFFECTS OF PULSED ELECTROMAGNETIC FIELD ON CoC2O4·2H2O POWDER SIZE[J]. Acta Metall Sin, 2009, 45(8): 1019-1024.
| [1] Roure SBouvard D, Dor´emus P, Pvier . Powder Metall, 1999; 42: 164
[2] Gillia O, Bouvard D. Mater Sci Eng, 2000; A279: 185
[3] Mao L , Shan Q, Yin S H, Liu B, Wu F. J Alloys Compd, 1999; 293–295: 825
[4] Liu Y, Zhu Y, Zhang Y, Qian Y, Zhang M, Yang L, Wang C. J Mater Chem, 1997; 7: 787
[5] Zheng Z S, Qu X H, Li Y P. Rare Met Mater Eng, 2004; 33: 393
(郑洲顺, 曲选辉, 李云平. 稀有金属材料与工程, 2004; 33: 393)
[6] Li Q H, Xiao W S, Liu Z H. Chin Powder Sci Technol, 2008; 18: 209
(李启厚, 肖松文, 刘志宏. 中国粉体技术, 2008; 18: 209)
[7] Liu S, Xu K, Wang M. Int J Refract Met Hard Mater, 2006; 24: 405
[8] Tikkanen M H, Taskinen A, Taskinen P. Powder Metall, 1975; 18: 259
[9] Huang P Y. Powder Metallurgy Principle. Beijing: Metallurgical Industry Press, 1982: 50
(黄培云. 粉末冶金原理. 北京: 冶金工业出版社, 1982: 50)
[10] Niu H L, Chen Q W, Zhu H F, Lin Y S, Zhang X. J Mater Chem, 2003; 13: 1803
[11] Wang F, Gu H Z, Zhang Z C. Mater Res Bull, 2003; 38: 347
[12] Wang J Z, Qi J G, Du H L, Zhang Z B. J Iron Steel Res Int, 2007; 14(4): 5
[13] Liu Z H. PhD Thesis, Central South University, Changsha, 2007
(刘志宏. 中南大学博士学位论文, 长沙, 2007)
[14] Randall M German. Powder Metallurgy Science. Princeton: Mtal Powder Industy, 1994: 168
[15] Liu Y H, Liu P A. Principle and Application of X–Ray Diffraction Analysis. Beijing: Chemical Industry Press, 2003: 212
(刘粤惠, 刘平安. X射线衍射分析原理与应用. 北京: 化学工业出版社, 2003: 212)
[16] Inorganic Chemistry Teaching and Research Section of Tianjin University. Inorganic Chemistry. Beijing: China Higher Education Press, 2002: 146
(天津大学无机化学教研室. 无机化学. 北京: 高等教育出版社, 2002: 146)
[17] Yao S T, Vekilov P G. Nature, 2000; 406: 494
[18] Shi E W, Chn , Yuan R L, Zheng Y Q. Hydrothermal Crystallography. Beijing: Science Press, 2004: 80
(施尔畏, 陈之战, 元如林, 郑燕青. 水热结晶学. 北京: 科学出版社, 2004: 80)
[19] Xu Y. Electromagnetics(Second Edition). Beijing: Science Press, 2004: 278
(徐 游. 电磁学(第二版). 北京: 科学出版社, 2004: 278)
[20] Chen S. PhD Thesis, Central South University, Changsha, 2003
(陈 松. 中南大学博士学位论文, 长沙, 2003) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|