金属学报  2009, Vol. 45 Issue (5): 615-619    
  论文 本期目录 | 过刊浏览 |
磁场沉积态FeCuCrVSiB薄膜的软磁特性和巨磁阻抗效应
陈卫平1;冯尚申1;邵先亦1;萧淑琴2;刘宜华2
1.浙江台州学院物理与电子工程学院; 台州 318000
2.山东大学物理学院; 济南250100
SOFT MAGNETIC PROPERTIES AND GIANT MAGNETOIMPEDANCE EFFECT IN MAGNETIC FIELD–DEPOSITED FeCuCrVSiB FILMS
CHEN Weiping1; FENG Shangshen1; SHAO Xianyi1;XIAO Shuqin2; LIU Yihua2
1.School of Physics and Electronics Engineering; Zhejiang Taizhou University; Taizhou 318000
2.School of Physics; Shandong University; Jinan 250100
引用本文:

陈卫平 冯尚申 邵先亦 萧淑琴 刘宜华. 磁场沉积态FeCuCrVSiB薄膜的软磁特性和巨磁阻抗效应[J]. 金属学报, 2009, 45(5): 615-619.
, , , , . SOFT MAGNETIC PROPERTIES AND GIANT MAGNETOIMPEDANCE EFFECT IN MAGNETIC FIELD–DEPOSITED FeCuCrVSiB FILMS[J]. Acta Metall Sin, 2009, 45(5): 615-619.

全文: PDF(537 KB)  
摘要: 

采用射频溅射法, 在无磁场和施加72 kA/m的纵向磁场下制备了FeCuCrVSiB软磁合金薄膜样品, 对沉积态样品的软磁特性和巨磁阻抗(GMI)效应进行了测量和分析. 结果表明, 在制备过程中加磁场可明显改善材料的软磁性能, 与无磁场沉积态相比, 样品的矫顽力从1.080 kA/m降低到0.064 kA/m, 在13 MHz频率下有效磁导率比从10%增加到106%. GMI效应与磁导率比的大小密切相关. 无磁场沉积态样品没有检测到GMI效应, 而磁场沉积态样品则具有显著的GMI效应. 在13 MHz 的频率下, 最大纵向和横向巨磁阻抗比分别高达22%和20%. 这些结果都优于厚度几乎相同的退火态FeCuNbSiB薄膜的GMI特性.

关键词 : FeCuCrVSiB薄膜,  巨磁阻抗效应,  软磁特性    
Abstract:

FeCuCrVSiB soft magnetic films have been prepared using radio frequency sputtering without or with a constant magnetic field of about 72 kA/m along the longitudinal direction of film plane, and then their soft magnetic properties and giant magnetoimpedance (GMI) effects were measured. The results obtained show that the magnetic field applied during the deposition process improves significantly the soft magnetic properties of the sample. For example, its coercive force decreases from 1.080 kA/m of the non–field–deposited state to around 0.064 kA/m and its effective permeability ratio increases from 10% to 106%. The GMI effect is closely connected with this permeability ratio. The GMI effect can not almost be detected in non–field–deposited samples, while it becomes evident for field–deposited samples. The maximum values of longitudinal and transverse GMI ratios are 22% and 20% at the frequency of 13 MHz, respectively. The GMI effect in the field–deposited sample is much better than in annealed FeCuNbSiB film with the same thickness.

Key words: FeCuCrVSiB film    giant magnetoimpedance effect    soft magnetic property
收稿日期: 2008-11-17     
ZTFLH: 

TG139

 
基金资助:

浙江省科技计划重点资助项目2006C21085

作者简介: 陈卫平, 女, 1954年生, 教授

[1] Panina L V, Makhnovskiy D P, Mohri K. J Magn Magn Mater, 2004; 272–276: 1452
[2] Ku´zmi´nski M, Nesteruk K, Lachowicz H K. Sens Actuators, 2008; 141A: 68
[3] Corrˆea M A, Viegas A D C, da Silva R B, de Andrade A M H, Sommer R L. J Appl Phys, 2007; 101: 043905
[4] Muraca D, Cremaschi V, Knobel M, Sirkin H. J Magn Magn Mater, 2008; 320: 2068
[5] Xin H L, Yuan W Z, Chen J K, Lin H, Ruan J Z, Zhao Z J. Acta Phys Sin, 2007; 56: 4152
(辛宏梁, 袁望治, 程金科, 林 宏, 阮建中, 赵振杰. 物理学报, 2007; 56: 4152)
[6] Amalou F, Gijs M A M. J Appl Phys, 2004; 95: 1364
[7] Yuan H M, Jiang S,Wang W J, Yan S S, Xiao S Q. Acta Metall Sin, 2006; 42: 971
(袁慧敏, 姜 山, 王文静, 颜世申, 萧淑琴. 金属学报, 2006; 42: 971)
[8] Xiao S Q, Liu Y H, Dai Y Y, Yan S S, Dai Y Y, Zhang L, Mei L M. Phys Rev, 2000; 61B: 5734
[9] Sommer R L, Chen C L. Appl Phys Lett, 1995; 67: 3346
[10] Yoshizawa Y, Yamauchi K. J Appl Phys, 1988; 64: 6044
[11] Zhang Y Z. Chin Sci Bull, 1993; 38: 2202
(张延忠. 科学通报, 1993; 38: 2202)
[12] Phan M H, Peng H X, Yu S C, V´azquez M. J Appl Phys, 2006; 99: 08C505

[1] 袁慧敏; 姜山; 王文静; 颜世申; 萧淑琴 . 制备态FeZrBNi/Ag/FeZrBNi三层膜的巨磁阻抗效应[J]. 金属学报, 2006, 42(9): 971-973 .
[2] 吴厚政; 刘宜华; 代由勇; 张林; 萧淑琴 . 磁场退火对CoFeNiNbSiB薄带巨磁阻抗的影响[J]. 金属学报, 2002, 38(10): 1087-1090 .
[3] 吴厚政; 刘宜华 . Co-Fe-Ni-Nb-Si-B非晶软磁合金薄带巨磁阻抗效应[J]. 金属学报, 2000, 36(9): 997-1000 .
[4] 刘德镇; 萧淑琴 . FeNiCrSiB/Cu/FeNiCrSiB膜的磁畴结构和巨磁阻抗效应[J]. 金属学报, 2000, 36(5): 535-538 .