| 环境介质对40Cr结构钢高周和超高周疲劳行为的影响 |
| 钱桂安; 洪友士 |
| 中国科学院力学研究所非线性力学国家重点实验室; 北京 100190 |
|
| EFFECTS OF ENVIRONMENTAL MEDIA ON HIGH CYCLE AND VERY-HIGH-CYCLE FATIGUE BEHAVIORS OF STRUCTURAL STEEL 40Cr |
| QIAN Gui'an; HONG Youshi |
| State Key Laboratory of Nonlinear Mechanics; Institute of Mechanics; Chinese Academy of Sciences; Beijing 100190 |
引用本文:
钱桂安 洪友士. 环境介质对40Cr结构钢高周和超高周疲劳行为的影响[J]. 金属学报, 2009, 45(11): 1356-1363.
,
.
EFFECTS OF ENVIRONMENTAL MEDIA ON HIGH CYCLE AND VERY-HIGH-CYCLE FATIGUE BEHAVIORS OF STRUCTURAL STEEL 40Cr[J]. Acta Metall Sin, 2009, 45(11): 1356-1363.
| [1] Stanzl S E, Tschegg E K, Mayer H. Int J Fatigue, 1986; 8: 195
[2] Kikukawa M, Ohji K, Ogura K. Trans ASME, 1965; 87D: 857
[3] Naito T, Ueda H, Kikuchi M. J Soc Materi Sci Jpn, 1983; 32: 1162
[4] Naito T, Ueda H, Kikuchi M. Metall Mater Trans, 1984; 15A: 1431
[5] Takeuchi E, Furuya Y, Nagashima N, Matsuoka S. Fatigue Fract Eng Mater Struct, 2008; 31: 599
[6] Ranc N, Wagner D, Paris P C. Acta Mater, 2008; 56: 4012
[7] Marines–Garcia I, Paris P C, Tada H, Bathias C, Lados D. Eng Fract Mech, 2008; 75: 1657
[8] Liu Y B, Yang Z G, Li Y D, Shen S M, Li S X, HuiWJ, Weng Y Q. Mater Sci Eng, 2008; A497: 408
[9] Gonzalo M, Dominguez A. Mech Mater, 2008; 40: 636
[10] Makino T. Int J Fatigue, 2008; 30: 1409
[11] Akiniwa Y, Stanzl–Tschegg S, Mayer H, Wakita M, Tanaka K. Int J Fatigue, 2008; 30: 2057
[12] Sohar C R, Betzwar–Kotas A, Gierl C,Weiss B, Danninger H. Int J Fatigue, 2008; 30: 1137
[13] Nakajima M, Tokaji K, Itoga H, Ko H N. Fatigue Fract Eng Mater Struct, 2003; 26: 1113
[14] Tokaji K, Ko H N, Nakajima M, Itoga H. Mater Sci Eng, 2003; A345: 197
[15] Furuya Y, Matsuoka S, Abe T, Yamaguchi K. Scr Mater, 2002; 46: 157
[16] Shiozawa K, Lu L. Fatigue Fract Eng Mater Struct, 2002; 25: 813
[17] Itoga H, Tokaji K, Nakajima M, Ko H N. Int J Fatigue, 2003; 25: 379
[18] Shiozawa K, Morii Y, Nishino S, Lu L. Int J Fatigue, 2006; 28: 1521
[19] Sakai T, Sato Y, Oguma N. Fatigue Fract Eng Mater Struct, 2002; 25: 765
[20] Zhou C E, Qian G A, Hong Y S. Key Eng Mater, 2006; 324–325: 1113
[21] Wang Q Y, Berard J Y, Rathery S, Bathias C. Fatigue Fract Eng Mater Struct, 1999; 22: 673
[22] McMahon Jr C J. Eng Fract Mech, 2001; 68: 773
[23] Taha A, Sofronis P. Eng Fract Mech, 2001; 68: 803
[24] Nagumo M, Shimura H, Chaya T, Hayashi H, Ochiai I. Mater Sci Eng, 2003; A348: 192
[25] Nagao A, Kuramoto S, Ichitani K, Kanno M. Scr Mater, 2001; 45: 1227
[26] Shipilov S A. Scr Mater, 2002; 47: 301
[27] Page R A, Gerberich W W. Met Trans, 1982; 13A: 305 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|