Please wait a minute...
金属学报  2007, Vol. 43 Issue (5): 503-508     
  论文 本期目录 | 过刊浏览 |
多元合金熔体组元活度系数计算方法的改进
蒋光锐;刘源;李言祥;苏彦庆;郭景杰
清华大学机械工程系材料加工技术研究所
Improvement of Calculation Method for the Activity Coefficient of Multi-component Alloys
Yuan Liu
清华大学机械工程系材料加工技术研究所
引用本文:

蒋光锐; 刘源; 李言祥; 苏彦庆; 郭景杰 . 多元合金熔体组元活度系数计算方法的改进[J]. 金属学报, 2007, 43(5): 503-508 .
, , , , . Improvement of Calculation Method for the Activity Coefficient of Multi-component Alloys[J]. Acta Metall Sin, 2007, 43(5): 503-508 .

全文: PDF(176 KB)  
摘要: 基于Miedema模型和Tanaka关系,提出了计算MIVM模型参数的新方法,开辟了计算多元合金熔体活度系数的新途径。分别计算了Ti-6Al-4V和Ti-5Al-2.5Sn在不同温度下组元活度系数的变化,计算了Zn-Sn-Pb-Cd-Bi合金活度系数与组元配比的关系,并与Wilson模型比较,计算值与实验值吻合较好。
关键词 : 多元合金,  活度系数,  Miedema模型    
Abstract:Based on the Miedema model and Tanaka equation, a new method for calculating the parameter of the Molecular Interaction Volume Model(MIVM) has been developed to get the activity coefficient of multi-component liquid alloys. The predicted activity coefficients of components in Ti-6Al-4V, Ti-5Al-2.5Sn and Zn-Sn-Pb-Cd-Bi alloys present a good agreement with the experimental data.
Key words: multi-component alloy    activity coefficient    Miedema model
收稿日期: 2006-09-04     
ZTFLH:  TG111.3  
[1] Wang H C, Dong Y C. Measurement and Calculation Methods of Metallurgical Thermodynamic Data. Beijing: Metallurgical Industry Press, 2005: 95 (王海川,董元篪.冶金热力学数据测定与计算方法.北京:冶金工业出版社,2005;95)
[2] Yue Q Z, Zhang X J, Cui J Z. Acta Metall Sin, 2003; 39: 35 (乐启炽,张新建,崔建忠.金属学报, 2003;39:35)
[3] Fan P, Zhou G Z. Acta Metall Sin, 1999; 35: 421 (范鹏,周国治.金属学报, 1999;35:421)
[4] Hardy H K. Acta Metall, 1953; 1: 202
[5] Wilson G M. J Am Chem Soc, 1964; 86: 127
[6] Prausnitz J M, Lichtenthaler R N,de Azevedo E G. Molecular Thermodynamics of Fluid-Phase Equilibria. 2nd ed., Englewood Cliffs, NJ: Prentice-Hall Inc., 1986: 193
[7] Renon H, Prausnitz J M. AIChE J, 1968; 14: 135
[8] Abrams D S, Prausnitz J M. AIChE J, 1975; 21: 116
[9] Gokcen N A. Statistical Thermodynamics of Alloys. New York: Plenum Press, 1986: 255
[10] de Boer F R. Cohesion in Metals: Transition Metal Alloys. Amsterdam: North-Holland, 1988: 1
[11] Miedema A R, de Chatel P F, de Boer F R. Physica, 1980; 1B: 1
[12] Chou K Z, Li W C, Li F S. CALPHAD, 1996; 20: 395
[13] Tao D P. Thermochim Acta, 2000; 363: 105
[14] Chen Z. Master Dissertation, Kunming University of Science and Technology, 2004 (陈卓.昆明理工大学硕士学位论文, 2004)
[15] Tao D P. Mater Sci Eng, 2005; A390: 70
[16] Tao D P. Metall Mater Trans, 2005; 36: 3495
[17] Tanaka T, Gokcen N A, Morita Z I. Z Metallkd, 1990; 81: 349
[18] Kong F Y, Yang K N. Acta Metall Sin, 1991; 27: B361 (孔凡亚,杨克努.金属学报, 1991;27:B361)
[19] Peng M, Mikula A. J Alloy Compd, 1997; 247: 185
[20] Peng M, Mikula A. Z Metallkd, 1995; 86: 4
[21] Oktay E. Z Metallkd, 1994; 85: 824
[22] Pang S M. Master Dissertation, Kunming University of Science and Technology, 2000 (庞思明.昆明理工大学硕士学位论文, 2000)
[23] Tao D P, Yang X W. Ada Metall Sin, 1997; 33: 1079 (陶东平,杨显万.金属学报, 1997;33:1079)
[1] 居天华, 舒念, 何维, 丁学勇. 合金溶液中溶质间活度相互作用系数预测模型[J]. 金属学报, 2023, 59(11): 1533-1540.
[2] 刘力恒,车淳山,孔纲,卢锦堂,张双红. 热镀Zn-0.2%Al镀层中Fe-Al抑制层失稳机理及其热力学评估*[J]. 金属学报, 2016, 52(5): 614-624.
[3] 郭金明; 郭喜平; 宋曙光 . Nb-Ti-Si基多元合金在1250 ℃下的氧化行为[J]. 金属学报, 2008, 44(5): 574-578 .
[4] 乐启炽; 张新建; 崔建忠; 路贵民 . 金属合金溶液热力学模型研究进展[J]. 金属学报, 2003, 39(1): 35-42 .
[5] 王玲玲; 黄维清 . 化学镀多元非晶态合金形成规律探讨[J]. 金属学报, 2002, 38(1): 84-90 .
[6] 侯怀宇; 谢刚 . 用NRTL方程预测三元,四元液态合金体系的热力学数据[J]. 金属学报, 1999, 35(3): 292-295 .
[7] 陈二保;董元篪;郭上型. Mn-Fe合金熔体热力学性质的研究[J]. 金属学报, 1997, 33(8): 831-837.
[8] 郭上型;董元篪. Fe-Mn-C-P系高锰熔体的热力学研究[J]. 金属学报, 1995, 31(18): 241-246.
[9] 蒋国昌;张晓兵;徐匡迪. C-Fe-X(X=Mn,Si,Cr,Ni)熔体中组元活度的解析[J]. 金属学报, 1992, 28(6): 52-58.
[10] 孔凡亚;杨克努;陆永安;孙树学. 钛合金液表层中合金元素浓度分布的研究[J]. 金属学报, 1991, 27(5): 141-143.
[11] 张千象. 固态Cu-Al合金中Al活度的测定[J]. 金属学报, 1989, 25(2): 149-151.
[12] 冀春霖;俞荣祥;刘素兰. Fe-B-Si三元系熔体的热力学 Ⅰ.1450℃时Si的活度及活度交互作用系数[J]. 金属学报, 1988, 24(2): 155-160.
[13] 冀春霖;俞荣祥;刘素兰. Fe-B-Si三元系熔体的热力学 Ⅱ.1450℃时硼的活度及活度交互作用系数[J]. 金属学报, 1988, 24(2): 161-165.