| 薄带双辊连铸水口电磁制动的实验模拟 |
| 李启胜;邓康;雷作胜; 李伟轩;任忠鸣 |
| 上海大学上海市钢铁冶金新技术开发应用重点实验室; 上海 200072 |
|
| Experimental Simulation of N--EMBr on Strip Casting with Twin Roll |
| LI Qisheng; DENG Kang; LEI Zuosheng; LI Weixuan; REN Zhongming |
| Shanghai Enhanced Laboratory of Ferro--Metallurgy; Shanghai University; Shanghai 200072 |
引用本文:
李启胜; 邓康; 雷作胜; 李伟轩; 任忠鸣 . 薄带双辊连铸水口电磁制动的实验模拟[J]. 金属学报, 2006, 42(7): 751-756 .
,
,
,
,
.
Experimental Simulation of N--EMBr on Strip Casting with Twin Roll[J]. Acta Metall Sin, 2006, 42(7): 751-756 .
[1] Li B Q.JOM,1995;47(5): 29 [2] Zapuskalov N. ISIJ Int, 2003, 43: 1115 [3] Wang X D.Master's Degree Thesis,Shanghai University, Shanghai,2004 (王晓东,上海大学硕士学位论文,上海, 2004) [4] Guthrie R I. L, Isac M. Steel Res,1999; 70: 343 [5] Kim D S,Kim W S,Kuznetsov A V.Numerical Heat Transfer, 2002; 41A: 1 [6] Seyedein S H,Hasan M. Numer Heat Transfer, 1997; 30A:221 [7] Jin Z M, Hao Y C, Xu G. Acta Matall Sin, 2000; 36 : 391 (金珠梅,赫翼成,徐 广.金属学报, 2000;36:391) [8] Miao Y C, Di H S, Zhang X M, Bao P W, Wang G D, Liu X H. Res Iron Steel, 2000; (2): 32 (苗雨川,邸洪双,张晓明,鲍培玮,王国栋,刘相华.钢铁研 究,2000;(2):32) [9] Bouchuard D, Busque F. 82nd steelmaking conference:1999 Proceedings, 1999: 427 [10] Wen G H, Zhu M M, He J F, Li G, Han Z W, Ding P D. Acta Metal Sin, 2000; 36 : 1001 (文光华,祝明妹,何俊范,李 刚,韩志伟,丁培道.金属学 报,2000;36:1001) [11] Chen F, Duan Z L,Wang W A.Experiments of Material Mechanics.Wuhan:Huazhong University of Science and Technology Press, 1999: 345 (陈锋,段自力,王文安.材料力学实验.武汉:华中理工大 学出版社,1999:133) [12] Hu H, Zhao H M, Zhang J M, Wang X H, Wang W J. Iron Steel Vanadium Titanium, 2005; 26 (1): 10 (胡皓,赵和明,张炯明,王新华,王万军.钢铁钒钛.2005; 26(1):10) [13] Huang W X, Chen W M. Engineering Hydrodynamics. Beijing: Chemical Industry Press, 2001: 65 (黄卫星,陈文梅.工程流体力学.北京:化学工业出版社,2001: 65) [14] Kollberq S G, Hackl H R,Hamley P J. Iron Steel Eng, 1996; 73 (7): 24 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|