| 不锈钢冶炼用AOD炉内的射流行为和流体流动 |
| 朱苗勇; 周海斌; 陈兆平; 黄宗泽 |
| 东北大学材料与冶金学院;沈阳110004 |
|
| BEHAVIORS OF JET AND FLUID FLOW IN AOD CONVERTER FOR STAINLESS STEEL REFINING |
| Zhu Miaoyong; Zhou Haibin; Chen Zhaoping; Huang Zongze |
| 沈阳市东北大学 |
引用本文:
朱苗勇; 周海斌; 陈兆平; 黄宗泽 . 不锈钢冶炼用AOD炉内的射流行为和流体流动[J]. 金属学报, 2006, 42(6): 653-656 .
,
,
,
.
BEHAVIORS OF JET AND FLUID FLOW IN AOD CONVERTER FOR STAINLESS STEEL REFINING[J]. Acta Metall Sin, 2006, 42(6): 653-656 .
[1] Asai S, Szekely J. Metall Trans,1974;5;651 [2] Fruehan R J. Ironmaking Steelmaking, 1976; 3:153 [3] Deb Roy T, Robertson D G. Ironmaking Steelmaking, 1978; 17: 198 [4] Themelis J, Tarassoff P, Szekely J. Trans Metall Soc AIME, 1969; 245: 2425 [5] Oryall G N, Brimacombe J K. Metall Trans, 1976; 7B: 391 [6] Hoefele E O, Brimacombe J K. Metall Trans, 1979; 10B: 631 [7] FigueiraR M, Szekely J. M,etall Trans,1985 10B: 67 [8] Xu K D. Stainless Steel Refining. Shanghai: Shanghai Science and Technology Press, 1985: 1 (徐匡迪.不锈钢精炼.上海:上海科学技术出版社,1985:1) [9] Wei J H, Zhu D P. Metall Mater Trans, 2001; 33: 121 [10] Fabritius T, Kupari P, Harkki .1. Scand J Metall, 2001; 30: 57 [11] Tillander A, Jonsson T L I, Jonsson P G. ISIJ Int. 2001; 41: 1156 [12] Zhu M Y, Sawada I, Iguchi M. ISIJ Int,1998;38;411 [13] Launder B E, Spalding D B. Mathematical Models of Turbulence. London: Academic Press, 1972: 1 [14] Patankar S V. Numerical Heat Transfer and Fluid Flow. New York: Hemisphere, 1980: 1 [15] Zhu M Y. Doctorate Thesis, Northeastern University, Shenyang, 1994 (朱苗勇.东北大学博士学位论文,沈阳, 1994) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|