| Ni76Cr19AlTi合金的热变形行为 |
| 滕浩; 尹志民; 朱远志; 周科朝; 李志友 |
| 中南大学材料科学与工程学院; 长沙 410083 |
|
| HOT DEFORMATION BEHAVIOR OF Ni76Cr19AlTi SUPERALLOY |
| TENG Hao; YIN Zhimin; ZHU Yuanzhi; ZHOU Kechao; LI Zhiyoue |
| 中南大学材料学院 |
引用本文:
滕浩; 尹志民; 朱远志; 周科朝; 李志友 . Ni76Cr19AlTi合金的热变形行为[J]. 金属学报, 2006, 42(6): 629-634 .
,
,
,
,
.
HOT DEFORMATION BEHAVIOR OF Ni76Cr19AlTi SUPERALLOY[J]. Acta Metall Sin, 2006, 42(6): 629-634 .
[1] Srinivasan N, Prasad Y V R K. J Mater Process Technol, 1995; 51: 171 [2] Choudhury I A, El-Baradie M A. J Mater Process Tech- nol, 1998; 77: 278 [3] Gabrisch H, Mukherji D. Acta Mater, 2000; 48: 3157 [4] Tian B, Paris O, Zickler G A, Lind C, Wasle G, May R P. Scr Mater, 2002; 47: 25 [5] Nembach E, Pesicka J, Langmaack E. Mater Sci Eng, 2003; A362: 264 [6] Kim D K, Kim D Y, Ryu S H, Kim D J. J Mater Process Technol, 2001; 113: 148 [7] Hagiwara Y, Ishida M, Oka T, Watanabe R, Sato K. SAE Trans, 1991; 100: 484 [8] Takagi Y, Oka.be M, Likubo T. Stahl Eisen, 1990; (Spec): 138 [9] Zener C, Hollomon J H. J Appl Phys, 1944; 15(1): 22 [10] Sellars C M. Acta Metall, 1966; 14: 1136 [11] Sellars C M, Tegart W J. Int Metall Rev, 1972; 17: 1 [12] Bruni C, Forcellese A, Gabrielli F. J Mater Process Technol, 2002; 125-126: 242 [13] Prasad Y V R K, Sasidhara S, Sikka V K. Intermetallics, 2000; 8: 987 [14] Park N K, Kim I S, Na Y S, Yeom J T. J Mater Process Technol, 2001; 111: 98 [15] Zhang B J, Zhao G P, Jiao L Y, Xu G H, Qin H Y, Feng D. Acta Metall Sin, 2005; 41: 351 (张北江,赵光普,焦兰英,胥国华,秦鹤勇,冯 涤.金属学 报,2005;41:351) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|