| 湿空气中恒磁场导致(Tb, Dy)Fe 2合金的滞后开裂 |
| 钮萼 |
| 北京科技大学材料物理系 |
|
| DELAYED CRACKING INDUCED BY CONSTANT MAGNETIC FIELD IN HUMID AIR FOR (Tb,Dy)Fe2 MAGNETOSTRICTIVE ALLOY |
| Niu E |
| 北京科技大学材料物理系 |
引用本文:
钮萼 . 湿空气中恒磁场导致(Tb, Dy)Fe 2合金的滞后开裂[J]. 金属学报, 2006, 42(4): 369-373 .
.
DELAYED CRACKING INDUCED BY CONSTANT MAGNETIC FIELD IN HUMID AIR FOR (Tb,Dy)Fe2 MAGNETOSTRICTIVE ALLOY[J]. Acta Metall Sin, 2006, 42(4): 369-373 .
[1] Engdahl G. In: Mayergoyz I ed, Handbook of Giant Mag-netostrictive Materials, New York: Academic Press, 2000: 1 [2] Wang B W. Preparation and Devices Design of Giant Magnetostrictive Materials. Beijing: Metallurgical Industry Press, 2003 (王博文.超磁致伸缩材料制备与器件设计.北京:冶金工业出 版社, 2003) [3] Wang B W, Yan R G. J Hebei Univ Technol, 2004; 33(2): 16 (王博文,闫荣格.河北工业大学学报, 2004;33(2):16) [4] Li K S, Li H W, Fang Y K. J Rare Earths, 2004; 22: 126 [5] Wang Y, Chu W Y, Su Y J, Qiao L J. Mater Sci Eng, 2002; B59: 263 [6] Wang Y, Chu W Y, Gao K W, Su Y J, Qiao L J. J Appl Phys, 2003; 82: 1583 [7] Yang W. Mechatronic Reliability. Beijing: Tsinghua University Press, 2001: 14 (杨 卫.力电失效学.北京:清华大学出版社, 2001:14) [8] Wang R M, Chu W Y, Gao K W, Su Y J, Qiao L J. Mater Lett, 2004; 58: 1811 [9] Wang R M, Chu W Y, Su Y J, Gao K W, Qiao L J. Acta Metall Sin, 2005; 41: 297 (王瑞敏,褚武扬,宿彦京,高克玮,乔利杰.金属学报,2005; 41:297) [10] Chu W Y, Qiao L J, Chen Q Z, Gao K W. Fracture and Environment Fracture. Beijing: Science Press, 2000: 6 (褚武扬,乔利杰,陈奇志,高克玮.断裂与环境断裂.北京: 科学出版社,2000:6) [11] Anstis G R, Chantikul P, Laun B R, Marshall D B. J Am Ceram Soc, 1981; 64: 533 [12] Chantikul P, Anstis G R, Laun B R, Marshall D B. J Am Ceram Soc, 1981; 64: 539 [13] Ma R Z, Jiang M H, Xu Z X. Functional Materials Generality. Beijing: Metallurgical Industry Press, 1999: 80 (马如璋,蒋民华,徐祖雄.功能材料学概论.北京:冶金工业 出版社,1999:80) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|