Please wait a minute...
金属学报  2006, Vol. 42 Issue (3): 280-284     
  论文 本期目录 | 过刊浏览 |
钢铁生产流程铁资源效率与工序铁资源效率关系的分析
戴铁军; 陆钟武
东北大学
THE ANALYSIS OF THE RELATIONSHIP BETWEEN IRON RESOURCE EFFICIENCY OF STEEL PRODUCTION PROCESS AND OF ITS UNIT PROCESS
daitiejun
引用本文:

戴铁军; 陆钟武 . 钢铁生产流程铁资源效率与工序铁资源效率关系的分析[J]. 金属学报, 2006, 42(3): 280-284 .
, . THE ANALYSIS OF THE RELATIONSHIP BETWEEN IRON RESOURCE EFFICIENCY OF STEEL PRODUCTION PROCESS AND OF ITS UNIT PROCESS[J]. Acta Metall Sin, 2006, 42(3): 280-284 .

全文: PDF(177 KB)  
摘要: 本文以钢铁生产流程铁流图为基础,推导了实际钢铁生产流程铁资源效率与工序铁资源效率的关系式。以某钢厂年均生产数据为例,分析了流程铁资源效率与工序铁资源效率的关系,并讨论了工序铁资源效率对流程铁资源效率的影响。
关键词 : 钢铁生产流程,  铁流图,  流程铁资源效率    
Abstract:Based on the concept of iron-flow diagram of steel production process, a relational expression between iron resource efficiency of steel production process and of its unit process has been derived. By using the data of a steel plant, the relationship between iron resource efficiency of steel production process and of its unit process was analyzed, and the influence of iron resource efficiency of unit process on iron resource efficiency of steel production process was discussed as examples.
Key words:
收稿日期: 2005-08-30     
ZTFLH:  TF089  
[1]Zhang S R.Res Iron Steel,2002;30(2):1 (张寿荣.钢铁研究,2002;30(2):1)
[2] Zhang X Y.Metall Manag,2003;(8):14 (张训毅.冶金管理, 2003;(8):14)
[3] Chen J B. Geol Seek, 2004; 19(1): 5 (陈甲斌.地质找矿论丛, 2004;19(1):5)
[4] Kleijn R. J Ind Ecol, 1999; 3(2, 3): 8
[5] Ayres R U. Resour Conseru Recycling, 1997; 21: 145
[6] Huang S L, Hsu W L. Landscape Urban Plann, 2003; 63: 61
[7] Fischer-Kowalski M. J Ind Ecol, 1998; 2(1): 61
[8] Fischer-Kowalski M, Hyttler W. J Ind Ecol, 1998; 2(4): 107
[9] de Marco O, Lagioia G, Mazzacane E P. J Ind Ecol , 2000; 4(2): 55
[10] Maenpaa I, Juutinen A. J Ind Ecol, 2001; 5(1): 33
[11] Spatari S, Bertram M, Fuse A K, Graedel T E, Rechberger H. Ecol Econo, 2002; 42: 27
[12] Hekkert M P, Joosten L A J, Worrell E. Resour Conser Recycling, 2000; 30: 29
[13] Michaelis P, Jackson T. Resour Conseru Recycling, 2000; 29: 131
[14] Michaelis P, Jackson T. Resour Conseru Recycling, 2000; 29: 209
[15] Yin R Y. Metallurgical Process Engineering. Beijing: Metallurgical Industry Press, 2004: 115 (殷瑞钰.冶金流程工程学.北京:冶金工业出版社,2004:115)
[16] Lu Z W, Cai J J, Yu Q B, Xie A G. Acta Metall Sin, 2000; 36: 370 (陆钟武,蔡九菊,于庆波,谢安国.金属学报,2000;36:370)
[17] Lu Z W. Acta Metall Sin, 2002; 38: 58 (陆钟武.金属学报,2002;38:58)
[18] Lu Z W, Dai T J. Iron Steel, 2005; 40(4): 1 (陆钟武,戴铁军.钢铁,2005;40(4):1)
[19] Dai T J, Lu Z W. Acta Metall Sin, 2004; 40: 1127 (戴铁军,陆钟武.金属学报,2004;40:1127)
[1] 戴铁军; 陆钟武 . 钢铁生产流程的铁流对铁资源效率的影响[J]. 金属学报, 2004, 40(11): 1127-1132 .
[2] 陆钟武 . 钢铁产品生命周期的铁流分析—关于铁排放量源头指标等问题的基础研究[J]. 金属学报, 2002, 38(1): 58-68 .
[3] 陆钟武 . 关于钢铁工业废钢资源的基础研究[J]. 金属学报, 2000, 36(7): 728-734 .
[4] 于庆波; 陆钟武 . 钢铁生产流程中物流对能耗影响的计算方法[J]. 金属学报, 2000, 36(4): 379-382 .