金属学报  2006, Vol. 42 Issue (12): 1259-1261     
  论文 本期目录 | 过刊浏览 |
温度诱导液态In-80%Sn合金结构非连续变化的分形分析
丁国华;祖方遒;余 谨;席 赟;张 燕
合肥工业大学材料学院
FRACTAL ANALYSIS OF TEMPERATURE-INDUCED DISCONTINUOUS LIQUID STRUCTURAL CHANGE
合肥工业大学材料学院
引用本文:

丁国华; 祖方遒; 余谨; 席赟; 张燕 . 温度诱导液态In-80%Sn合金结构非连续变化的分形分析[J]. 金属学报, 2006, 42(12): 1259-1261 .

全文: PDF(512 KB)  
摘要: 用分形理论探讨了液态In-80%Sn结构及其变化, 证实了液体结构中存在分形结构, 发现随着温度的升高, 与液态合金其它结构参数一样, 分形维数也发生了不连续的变化, 提出分形维数是一个结构敏感参量. 分析认为液态In-Sn合金结构所出现的不连续变化是由于液体中粒子集合体线度减小而出现的线度效应所造成的, 分形维数的突变是温度诱导液态结构不连续的基本特性.
关键词 : 液态合金结构,  分形理论,  温度诱导结构变化    
Abstract:As a new and important problem in condensed state physics, the discontinuous structural change of liquid with temperature rising is testified by various experimental technologies. However, fractal language has been more and more frequently used to describe some disordered physical systems except liquid alloys. This paper has successfully implemented fractal ideas to observe fractal structures in liquid In-Sn alloy and considers its fractal dimension as a physical quantity sensitive to structure. Moreover, from the fractal viewpoint, the mutation of the fractal dimension has indicated once again that the liquid structure change discontinuously with temperature rising.
Key words: liquid alloys structure    fractal theory    temperature-induced
收稿日期: 2006-04-04     
ZTFLH:  O552.41  
[1] Gefen Y, Mandelbrot B B. Phys Rev Lett, 1980; 45: 855
[2] Zu F Q, Zhu Z G, Guo L J, Zhang B, Shui J P, Liu C S. Phys Rev, 2001; 64B: 180203
[3] Zu F Q, Zhu Z G, Guo L J, Qin X B, Yang H, Shan W J. Phys Rev Lett, 2002; 89: 125505
[4] Li X F, Zu F Q, Ding H F, Yu J, Liu L J, Li Q, Xi Y. Physica, 2005; 358B: 126
[5] Wang L, Bian X F, Liu J T. Phys Lett, 2004; 326A: 429
[6] Waseda Y. The Structure of Non-Crystalline Materials. New York: McGraw-Hill, 1980: 1
[7] Chu W Y, Su Y J, Gao K W, He J Y, Li J X, Qiao L J. Fractals in Materials Science. Beijing: Chemical Industry Press, 2004: 63 (楮武扬,宿彦京,高克玮,何健英,李金许,乔利杰.材料科学中的分形.北京;化学工业出版社,2004:63)
[8] Yang Z R. Fractal Physics. Shanghai: Shanghai Scientific and Technological Education Publishing House, 1996: 4 (杨展如.分形物理学.上海:上海科技教育出版社, 1996:4)
[9] Elliott S R. Nature, 1991; 354: 445
[10] Deng Z J. Ultrafine Particle and Fractal. Chongqing: Southwest China Normal University Press, 1993: 1 (邓昭镜.超微粒与分形.重庆:西南师范大学出版社, 1993: 1)
[11] Bian X F, Liu X F, Ma J J. Heredity in Cast Metals. Jinan: Shandong Science & Technology Press, 1998: 1 (边秀房,刘相法,马家骥.铸造金属遗传学.济南:山东科学技术出版社,1998:1)
No related articles found!