| 纳米金属微粒二元相图的尺寸效应和形状效应 |
| 齐卫宏 |
| 江苏大学材料科学与工程学院; 镇江 212013 |
|
| Size and Shape Dependent Phase Diagram of Binary Metallic Nanoparticles |
| QI Weihong |
| School of Materials Science and Engineering; Jiangsu University; Zhenjiang 212013 |
引用本文:
齐卫宏 . 纳米金属微粒二元相图的尺寸效应和形状效应[J]. 金属学报, 2006, 42(1): 73-76 .
.
Size and Shape Dependent Phase Diagram of Binary Metallic Nanoparticles[J]. Acta Metall Sin, 2006, 42(1): 73-76 .
[1]Wautelet M,Dauchot J P,Hecq M.Mater Sci Eng,2003;C23:187 [2]Wautelet M,Dauchot J P,Hecq M.Nanotechnology,2000;11:6 [3]Lai S L,Guo J Y,Petrova V.Phys Rev Lett,1996;77:99 [4]Eckert J,Holzer J C,Ahn C C,Fu Z,Johnson W L.Nanostruct Mater,1993,2:407 [5]Jiang Q,Yang C C,Li J C.Mater Lett,2002;56:1019 [6]Xu ZY,Li L.Thermodynamics of Material.Beijing:Science Press,2001:148(徐祖耀,李麟.材料热力学.北京:科学出版社,2001:148) [7]Qi W H,Wang M P.Chem Phys Lett,2003;372:632 [8]Qi W H,Wang M P.Mater Chem Phys,2004;88:280 [9]Kim H K,Huh S H,Park J W,Jeong J W,Lee G H.Chem Phys Lett,2002;354:165 [10]Rose J H,Ferrante J,Smith J R.Phys Rev Lett,1981;47:675 [11]Mott N F.Proc Roy Soc Lond,1934;146A:465 [12]Regel A R,Glazov V M.Semiconductors,1995;29:405 [13]Ubbelohde A R.Melting and Crystal Structure.Oxford:Clarendon Press,1965:88 [14]Zhang Z,Lu X X,Jiang Q.Physica,1999;B270:249 [15]Hou Z S,Lu G X.Principle of Metallography.Shanghai:Shanghai Technology and Science Press,1990:63(侯增寿,卢光熙.金属学原理.上海:上海科学技术出版社,1990:63) [16]Nanda K K,Sahu S N,Behera S N.Phys Rev,2002;66A:013208 [17]Brandes E A.Smithells Metals Rreference Book.6th ed.London:Butterworths,1983:8 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|