| 计算Fe--C--Xi合金系在正平衡和准平衡模式下相变驱动力的简便方法 |
| 盛 广 杨志刚 |
| 清华大学材料科学与工程系; 北京 100084 |
|
| A Simple Calculation Method of Driving Force of Transformation in Fe--C--Xi Systems with Orthoequilibrium and Paraequilibrium Models |
| SHENG Guang; YANG Zhigang |
| Department of Materials Science and Engineering; Tsinghua University; Beijing 100084 |
引用本文:
盛广; 杨志刚 . 计算Fe--C--Xi合金系在正平衡和准平衡模式下相变驱动力的简便方法[J]. 金属学报, 2006, 42(1): 23-27 .
,
.
A Simple Calculation Method of Driving Force of Transformation in Fe--C--Xi Systems with Orthoequilibrium and Paraequilibrium Models[J]. Acta Metall Sin, 2006, 42(1): 23-27 .
[1]Tanaka T,Aaronson H I,Enomoto M.Metall Mater Trans,1995;26A:547 [2]Purdy G R,Weichert D H,Kirkaldy J S.Trans Met Soc AIME,1964;230:1025 [3]Hillert M.The Mechanism of Phase Transformations in Crystalline Solids.London:Inst of Metals,1969;33:231 [4]Aaronson H I,Domian H A.Trans Met Soc AIME,1966;236:768 [5]Enomoto M,Aaronson H I.Scr Metall,1985;19:1 [6]Gilmour J B,Purdy G R,Kirkaldy J S.Metall Trans,1972;3:1455 [7]Gilmour J B,Purdy G R,Kirkaldy J S.Metall Trans,1972;3:3213 [8]Hillert M.Yernkontorets Ann,1952;136:25 [9]Hultgren A.Jernkontorets Ann,1951;135:403 [10]Rudberg E.Jernkontorets Ann,1952;136:91 [11]Russel K C.Phase Transformations.Metals Park,OH:ASM,1970:219 [12]Hillert M.Lectures on the Theory of Phase Transformation.Warrendale,PA:TMS-AIME,1975:1 [13]Enomoto M,Aaronson H I.Metall Trans,1986;17A:1381 [14]Porter D A,Easterling K E.Phase Transformation in Metals and Alloys.Berkshire,England:Van Nostrand Reinhold(UK)Co.Ltd.,1981:11 [15]Kirkaldy J S,Baganis E A.Metall Trans,1978;9A:495 [16]Wanger C.Thermodynamics of Alloys.Reading,Mass:Addision-Westey,1952:88 [17]Offerman S E,van Dijk S H,Sietsma J,Grigull S,Lauridsen E M,Margulies L,Poulsen H F,Rekveldt M Th,van der Zwaag S.Science,2002;298:1003 [18]Oi K,Lux C,Purdy G R.Acta Mater,2000;48:2147 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|