| Fe-66.7%Si合金液滴落管实验的动力学和传热学计算 |
| 王海燕 刘日平 战再吉 孙力玲 王文魁 |
| 燕山大学亚稳材料制备技术与科学重点实验室;秦皇岛 066004; 中国科学院物理研究所;北京 100080 |
|
| DYNAMIC AND THERMAL COMPUTATION OF Fe-66.7%Si DROPLETS FREE FALLING IN A DROP TUBE |
| WANG Haiyan; LIU Riping; ZHAN Zaiji; SUN Liling |
引用本文:
王海燕; 刘日平; 战再吉; 孙力玲; 王文魁 . Fe-66.7%Si合金液滴落管实验的动力学和传热学计算[J]. 金属学报, 2005, 41(9): 940-946 .
,
,
,
,
.
DYNAMIC AND THERMAL COMPUTATION OF Fe-66.7%Si DROPLETS FREE FALLING IN A DROP TUBE[J]. Acta Metall Sin, 2005, 41(9): 940-946 .
[1] Tani J, Kido H. J Appl Phys, 1999; 86: 464 [2] Leong D, Harry M, Reason K J, Homewood K P. Nature, 1997; 387: 686 [3] Kubaschewski O. Iron-Binary Phase Diagram. Berlin: Springer, 1982: 138 [4] Yamauchi I, Ueyama S, Ohnaka I. Mater Sci Eng, 1996; A208: 108 [5] Yamauchi I, Nagase T, Ohnaka I. J Alloy Compd, 1999; 292: 181 [6] Yamauchi I, Okamoto T, Ohata H, Ohnaka I. J Alloy Compd, 1997; 260: 162 [7] McCoy J K, Markworth A J, Brodkey R S, Collings E W. Mater Res Soc Symp Proc, 1987; 87: 163 [8] Evans N D, Hofmeister W H, Bayuzick R J, Robinson M B. Metall Trans, 1986; 17A: 973 [9] Lacy L L, Robinson M B, Evans N D, Bayuzick R J, Rathz T J. Mater Res Soc Symp Proc, 1982; 9: 87 [10] Pan M X, Chen X C. Physics, 1988; 17: 475 (潘明祥,陈熙琛.物理, 1988;17:475) [11] Cliff R, Grace J R, Weber M E. Bubbles, Drops and Particles. New York: Academic Press, 1978: 111 [12] Brazhkin V V, Larchev V I, Popova S V, Skrotskaya G G. Phys Scr, 1989; 39: 338 [13] White F M. Viscous Fluid Flow. New York: McGrawHill, 1974: 35 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|