| 基于串热源及CCT图的GMAW焊接热影响区组织及硬度预测 |
| 王后孝 魏艳红 孙俊生 郑媛媛 |
| 哈尔滨工业大学现代焊接生产技术国家重点实验室; 哈尔滨 150001 |
|
引用本文:
王后孝; 魏艳红; 孙俊生; 郑媛媛 . 基于串热源及CCT图的GMAW焊接热影响区组织及硬度预测[J]. 金属学报, 2005, 41(8): 839-846 .
[1] Song T H. In: The 8th Chinese Welding Conference on Development of Advanced Production and the Future of Welding Technology (Vol.1), Beijing: China Machine Press, 1997: 17 (宋天虎.第八次全国焊接会议论文集(第1册).北京:机械工 业出版社,1997:17) [2] Dithey U. In: Proc. of HW Asian-Pacific Welding Conference on Capabilities of Welding Processes and Their Automation Potential with A View to the Year 2000, Auckland, New Zealand, 1996: 65 [3] Wang H X, Hua P, Sun J S, Yang Z D. J Shandong Univ (Eng Sci), 2004; 34(1): 25 (王后孝,华鹏,孙俊生,杨致东.山东大学学报(工学版), 2004,34(1):25) [4] Wang H X, Sun J S., J Shandong Jiaotong Univ, 2003; 11(4): 35 (王后孝,孙俊生.山东交通学院学报, 2003;11(4):35) [5] Rosenthal D, Ambridge M G. Trans ASME, 1946; 68: 849 [6] Rykalin N N. Calculations of Thermal Processes in Welding. Moscow: Mashgiz Publishing, 1951: 3 [7] Eager T W, Tsai N S. Weld J, 1983; 62: 346 [8] Kasuya T, Yurioka N. Weld J, 1993; 72: 107 [9] Nguyen N T, Ohta A, Matsuokak K, Suzuki N, Maeda Y. Weld J, 1999; 78: 265 [10] Moon D W, Lambrakos S G, Wong R J, Metzbower E A. Sci Technol Weld Joining, 2003; 8: 334 [11] Zhang W, Elmer J W, Debroy T. Mater Sci Eng, 2002; A333: 320 [12] Wang H X, Sun J S, Wei Y H, Zheng Y Y. Sci Technol Weld Joining, 2005, in press [13] Cao Z, Brust F, Nanjundan A, Dong Y, Julta T. In: The 2000 ASME Pressure Vessels and Piping Conference, 410(1), Seattle, 2000: 37 [14] Wang H X. Master's Thesis, Shandong University, Jinan, 2004 (王后孝.山东大学硕士学位论文,济南, 2004) [15] Wu C S. Numerical Analysis for Welding Thermal Process. Harbin: Harbin Institute of Technology Press, 1990: 25 (武传松.焊接热过程数值分析.哈尔滨:哈尔滨工业大学出版 社,1990:25) [16] Wu C S, Sun J S. In: Proc Inst Mech Eng, 1998; 212B: 525 [17] Zhang W Y. Physical Metallurgy of Welding Process. Beijing: China Machine Press, 1997: 168 (张文钺.焊接冶金学.北京:机械工业出版社, 1997:168) [18] Michio I. Welding Technology (Machinery Method 3). Tokyo: Seibundo Shinkosha, 1971: 6 (稻垣道夫.溶接加工(机械工作法3).东京:诚文堂新光社, 1971:6) [19] Chen B G, Zhang W Y, Du Z Y, Xu Y H. In: The 4th Chinese Welding Conference on the Parameter Measurement for Thermal Cycles During Bolt Experiments, H-IXa-029-81, 1980 (陈邦固,张文钺,杜则裕,许玉环.第四届焊接年会论文,H— IXa-029—81,1980) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|