| 等轴应变作用下Cu, Al薄膜的取向择优生长 |
| 周耐根 周 浪 宋固全 宋照东 |
| (南昌大学材料科学与工程学院; 南昌 330047) |
|
引用本文:
周耐根; 周浪; 宋固全; 宋照东 . 等轴应变作用下Cu, Al薄膜的取向择优生长[J]. 金属学报, 2005, 41(8): 809-813 .
[1] Rosenberg R, Edelstein D C, Hu C K, Rodbell K P. Ann Rev Mater Sci, 2000; 30: 229 [2] Stearns M B, Lee C H, Chang OH, Petford-long A K. In: Hong M, Wolf S, Gubser D C eds., Metallic Multilayers and Epitaxy, Warrendale, PA: TMS, 1988: 55 [3] Smith D L. Thin-Film Deposition. New York: McGraw Hill Inc, 1995: 165 [4] Liu W C, Huang H C. Comput Mater Sci, 2002; 23: 155 [5] Zhou N G, Zhou L. Acta Metall Sin, 2004; 40: 897 (周耐根,周浪.金属学报,2004;40:897) [6] Zhou N G, Zhou L. Acta Phys Sin, 2005 (in Press) (周耐根,周 浪.物理学报, 2005,待发表) [7] Ying F, Smith R W, Srolovitz D J. Appl Phys Lett, 1996; 69: 3007 [8] Dong L, Srolovitz D J. J Appl Phys, 1998; 84: 5261 [9] Zhou L, Zhou N G, Zhu S L. Acta Metall Sin, 2002; 38: 7.95 (周 浪,周耐根,朱圣龙.金属学报, 2002;38:795) [10] Zhou L, Zhu S L. Scr Mater, 2002; 47: 677 [11] Ackland G J, Tichy G, Vitek V, Finnis M W. Philos Mag, 1987; 56A: 735 [12] Ercolessi F, Adams J. Europhys Lett, 1994; 26: 583 [13] Zhou L, Wei X Q, Zhou N G. Comput Mater Sci, 2004; 30: 314 [14] Peng B, Cai M, Li G, Wu X J, Zhou F. Nanostruct Mater, 1994; 4: 475 [15] Bockstedte M, Liu S J, Huang H C. Comput Mater Sci, 2002; 23: 85 [16] Toxvared S. Phys Rev, 1993; E47: 343 [17] Zhou X W, Johnson R A, Wadley H N G. Acta Mater, 1997; 45: 1513 [18] Feng D. Physics of Metals. Beijing: Science Press, 1998: 333 (冯端.金属物理学.北京:科学出版社, 1998:333) [19] Gerold V, Translated by Wang P X. Structure of Solids. Beijing: Science Press, 1998: 393 (Gerold V著,王佩璇译.固体结构.北京:科学出版社,1998: 393) [20] Watanabe T, Tsurekawa S. Acta Mater, 1999; 47: 4171 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|