形变温度对中碳钢组织转变的影响
惠卫军;田 鹏;董 瀚;苏世怀;于同仁;翁宇庆
钢铁研究总院结构材料研究所; 北京 100081; 马鞍山钢铁股份有限公司; 马鞍山 243000
Influence of Deformation Temperature on the Microstructure Transformation in Medium Carbon Steel
HUI Weijun; TIAN Peng; DONG Han; SU Shihuai; YU Tongren; WENG Yuqing
Institute of Structural Materials; Central Iron & Steel Research Institute; Beijing 100081; Ma'anshan Iron & Steel Co. Ltd.; Ma'anshan 243000
引用本文:

惠卫军; 田鹏; 董瀚; 苏世怀; 于同仁; 翁宇庆 . 形变温度对中碳钢组织转变的影响[J]. 金属学报, 2005, 41(6): 611-616 .
, , , , , . Influence of Deformation Temperature on the Microstructure Transformation in Medium Carbon Steel[J]. Acta Metall Sin, 2005, 41(6): 611-616 .

全文: PDF(417 KB)  
摘要: 热模拟单向压缩下中碳钢形变温度低于Ad3 (786 ℃)点时, 析出形变诱导铁素体(DIF), DIF量随形变温度 降低而提高; 在低于750 ℃形变时, DIF量远高于平衡 态铁素体含量54%. DIF析出时碳原子高度富集在铁素体晶界 和铁素体/奥氏体界面. 在低于A1 (719 ℃)等温处理时, 高于Ad3点形变试样中, 奥氏体转变为铁素体+片层状珠光体; 低于Ad3点但高于Ar3 (645 ℃)点形变时, 未转变奥氏体转变为铁素体+片层状珠光体+晶界渗碳体; 稍高于Ar3点形变时, 将获得铁素体+弥散渗碳体的球化组织.
关键词 : 形变温度,  中碳钢,  组织转变    
Abstract:During uniaxial hot compression for a medium carbon steel, the deformation induced ferrite (DIF) appeared when deformed temperatures lower than A d3 (786 ℃). The volume fraction of DIF increases with decreasing deformation temperature, especially when deformed temperatures lower than 750 ℃ the volume fraction of DIF increases significantly, which is far beyond the equilibrium ferrite fraction of 54%. With the increase of DIF, more and more carbon atoms were rejected into the boundaries of ferrite and interfaces of ferrite/untransformed austenite. During isothermal holding below A1 (719 ℃) temperature just after deformation, supercooled austenite would decompose to different structures in three different ways: when the deformation temperature is higher than Ad3, conventional ferrite-lamellar pearlite structure was obtained; when the deformation temperature is lower than Ad3 whereas higher than Ar3 (645 ℃), retained austenite transformed to ferrite-lamellar or degenerated pearlite-grain boundary cementite; when the deformation temperature decreased to just above Ad3, a microstructure different from lamellar pearlite was obtained, which consisted of fine cementite particle and ferrite.
Key words: deformation temperature    medium carbon steel    microstructure evolution
收稿日期: 2004-09-15     
ZTFLH:  TG111  
[1]Weng Y Q.Iron Steel,2003;38(5):1 (翁宇庆.钢铁,2003;38(5);1)
[2]Tsuji N.Tetsu Hagane,2002;88:359 (辻伸泰.铁之钢,2002;88:359)
[3]Li W J,Wang G D,Liu X H.In:Workshop on New Generation Steel (NG Steel'2001),Beijing:The Chinese Society for Metals,2001:311 (李维娟,王国栋,刘相华.见:新一代钢铁材料研讨会,北京,中国金属学会,2001:311)
[4]Tian Z X,Yang P,Sun Z Q.Trans Mater Heat Treat,2003;24(3):18 (田朝旭,杨平,孙祖庆.材料热处理学报,2003;24(3):18)
[5]O'Brien J M,Hosford W F.Metall Mater Trans,2002;33A:1255
[6]Park J,Song D H,Lee D,Choo W Y.In:Zhu Y T,Lang-don T G,Mishra R S,Semiatin S L,Saran M J,Lowe T C,eds.,Ultrafine Grained Materials Ⅱ,Seattle:The Minerals,Metals & Materials Society,2002:275
[7]Storojeva L,Kaspar R,Ponge D.Mater Sci Forum,2003;426-432:1169
[8]Weng Y Q,et al.Ultrafine Grained Steels-The Theory of Microstructure Refinement and Controlling Technology for Steels.Beijing:Metallurgical Industry Press,2003:140,118 (翁宇庆,等.超细晶钢——钢的组织细化理论与控制技术.北京,冶金工业出版社,2003:140,118)
[9]McQueen H J,Ryan N D.Mater Sci Eng,2002;A322:43
[10]An Y Z.Heat Treatment Technology.Beijing:China Machine Press,1982:51 (安运铮.热处理工艺学.北京:机械工业出版社,1982:51)
[1] 王周头, 袁清, 张庆枭, 刘升, 徐光. 冷轧中碳梯度马氏体钢的组织与力学性能[J]. 金属学报, 2023, 59(6): 821-828.
[2] 武慧东, 宫本吾郎, 杨志刚, 张弛, 陈浩, 古原忠. Fe-1.5(3.0)%Si-0.4%C合金贝氏体不完全转变现象及伴随的渗碳体析出[J]. 金属学报, 2018, 54(3): 367-376.
[3] 徐滨士,方金祥,董世运,刘晓亭,闫世兴,宋超群,夏丹. FV520B不锈钢激光熔覆热影响区组织演变及其对力学性能的影响*[J]. 金属学报, 2016, 52(1): 1-9.
[4] 吴斯, 李秀程, 张娟, 尚成嘉. Nb对中碳钢相变和组织细化的影响*[J]. 金属学报, 2014, 50(4): 400-408.
[5] 王斌,刘振宇,周晓光,王国栋. 轧后冷却路径对中碳钢扩孔性能的影响[J]. 金属学报, 2012, 48(4): 435-440.
[6] 彭云 王爱华 肖红军 田志凌. Cu对690 MPa级HSLA钢熔敷金属组织形成和细化的作用[J]. 金属学报, 2012, 48(11): 1281-1289.
[7] 李龙飞, 夏杨青, 孙祖庆, 杨王玥 . 中碳钢回火马氏体热变形过程中的铁素体动态再结晶[J]. 金属学报, 2010, 46(1): 19-26.
[8] 张寒 白秉哲. Mn-Si-Cr系中碳钢在过冷奥氏体状态下变形时的显微组织演变[J]. 金属学报, 2010, 46(1): 47-51.
[9] 张继旺 鲁连涛 张卫华. 微粒子喷丸中碳钢疲劳性能分析[J]. 金属学报, 2009, 45(11): 1378-1383.
[10] 陈国安; 杨王玥; 孙祖庆; 张湘义 . 中碳钢过冷奥氏体形变过程中碳的分布与扩散[J]. 金属学报, 2007, 43(8): 785-790 .
[11] 陈国安; 杨王玥 . 中碳钢过冷奥氏体形变过程的组织演变[J]. 金属学报, 2007, 42(1): 27-34 .
[12] 姚可夫; 钱滨; 石伟; 刘春成; 刘庄 . 马氏体回火过程中组织转变量预测的实验研究[J]. 金属学报, 2003, 39(8): 892-896 .
[13] 董祥林; 简小刚; 毕红运; 陈金荣 . 磁场对中碳钢滑动摩擦磨损的影响[J]. 金属学报, 1999, 35(6): 577-580 .
[14] 张奎; 张永忠 . 半固态AlSi7Mg合金二次加热工艺与组织转变机制[J]. 金属学报, 1999, 35(2): 127-130 .
[15] 殷为民; 郭建宁; V.Lupinc . 铸造TiAl-W-Si合金的组织转变[J]. 金属学报, 1999, 35(1): 32-36 .