|
|
|
| SS304不锈钢在室温单轴循环加载下的时相关棘轮行为 |
| 康国政;孙亚芳;张娟;阚前华 |
| 西南交通大学应用力学与工程系; 成都 610031 |
|
| Time-Dependent Ratcheting Behavior of SS304 Stainless Steel Under Uniaxial Cyclic Loading at Room Temperature |
| KANG Guozheng; SUN Yafang; ZHANG Juan; KAN Qianhua |
| Department of Applied Mechanics and Engineering; Southwest Jiaotong University; Chengdu 610031 |
引用本文:
康国政; 孙亚芳; 张娟; 阚前华 . SS304不锈钢在室温单轴循环加载下的时相关棘轮行为[J]. 金属学报, 2005, 41(3): 277-281 .
,
,
,
.
Time-Dependent Ratcheting Behavior of SS304 Stainless Steel Under Uniaxial Cyclic Loading at Room Temperature[J]. Acta Metall Sin, 2005, 41(3): 277-281 .
[1] Chaboche J L, Nouailhas D. ASME J Eng Mater Technol, 1989; 111: 384 [2] Ruggles M D, Krempl E. J Mech Phys Solids, 1990; 38: 575 [3] Delobelle P, Robinet P, Bocher L. Int J Plast, 1995; 11: 295 [4] McDowell D L. Int J Plast, 1995; 11: 397 [5] Kobayashi M, Ohno N, Igari T. Int J Plast, 1998; 14: 355 [6] Mizuno M, Mima Y, Abdel-Karim M, Ohno N. ASME J Eng Mater Technol, 2000; 122: 29 [7] Kang G Z, Gao Q, Cai L X, Yang X J, Sun Y F. Acta Metall Sin, 2000; 36: 497 (康国政,高庆,蔡力勋,杨显杰,孙亚芳.金属学报,2000; 35:497) [8] Kang G Z, Gao Q, Yang X J, Sun Y F. J Mater Sci Tech- nol, 2001; 17: 219 [9] Kang G Z, Gao Q, Cai L X, Sun Y F. Nucl Eng Des, 2002; 216: 13 [10] Kang G Z, Gao Q, Yang X J. Int J Mech Sci, 2002; 44: 1645 [11] Chaboche J L. Int J Plast, 1991; 7: 661 [12] Delobelle P. Int J Plast, 1993; 9: 65 [13] Ohno N, Wang J D. Int J Plast, 1993; 9: 375 [14] Yoshida F. Eur J Mech A-Solids, 1995; 14: 97 [15] Jiang Y, Sehitoglu H. ASME J Appl Mech, 1996; 63: 720 [16] Ohno N, Abdel-Karim M. ASME J Eng Mater Technol, 2000; 122: 35 [17] Bari S, Hassan T. Int J Plast, 2002; 18: 873 [18] Kang G Z, Gao Q, Yang X J. Mech Mater, 2002; 34: 521 [19] Gao Q, Kang G Z, Yang X J. Theor Appl Fract Mech, 2003; 40: 105 [20] Kang G Z. Mech Mater, 2004; 36: 299 [21] Kang G Z, Ohno N, Nebu A. Int J Plast, 2003; 19: 1801 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|