| 高频调幅磁场下无结晶器振动电磁连铸技术的实验研究 |
| 雷作胜 任忠鸣 闫勇刚 邓康 |
| 上海大学上海市钢铁冶金新技术应用开发重点实验室; 上海 200072 |
|
| Experimental Study on Mold Oscillation-Less Continuous Casting Process Under High Frequency Amplitude-Modulated Magnetic Field |
| LEI Zuosheng; REN Zhongming; YAN Yonggang; DENG Kang |
引用本文:
雷作胜; 任忠鸣; 闫勇刚; 邓康 . 高频调幅磁场下无结晶器振动电磁连铸技术的实验研究[J]. 金属学报, 2004, 40(9): 995-999 .
,
,
,
.
Experimental Study on Mold Oscillation-Less Continuous Casting Process Under High Frequency Amplitude-Modulated Magnetic Field[J]. Acta Metall Sin, 2004, 40(9): 995-999 .
[1] Asai S. Tetsu Hagane, 1989; 75: 32(浅井滋生.铁 钢,1989;75:32) [2] Ren Z M, Dong H F, Deng K. ISIJ Int, 2001; 41: 981 [3] Li T J, Sassa K, Asai S. ISIJ Int, 1996; 36: 410 [4] Zhou Y M, Sassa K, Asai S. Tetsu Hagane, 1999; 85: 460(周月明,佐佐健介,浅井滋生.铁 钢,1999;85:460) [5] Su Z J, Iwai K, Asai S. CAMP-ISIJ, 1998; 11: 132 (苏志坚,岩井一彦,浅井滋生.材料 ,1998;11:132) [6] Su Z J, Iwai K, Asai S. ISIJ Int, 1999; 39: 1224 [7] Zhou Y M, Sassa K, Asai S. Acta Metall Sin, 2001; 37:777(周月明,佐佐健介,浅井滋生.金属学报, 2001;37:777) [8] Lei Z S, Ren Z M, Deng K. Chin J Nonferrous Met, 2002; 12 (Suppl.1) : 30(雷作胜,任忠鸣,邓康.中国有色金属学报,2002;12(增刊1) :30) [9] Dong H F, Ren Z M, Zhong Y B, Deng K. J Iron Steel Res, 1998; 10: 5(董华峰,任忠鸣,钟云波,邓康.钢铁研究学报,1998;10:5) [10] Sassa K, Li T J, Asai S. Tetsu Hagane, 1993, 79: 1075(佐佐健介,李廷举,浅井滋生.铁 钢, 1993;79:1075) [11] Zhou Y M, Sassa K, Asai S. Acta Metall Sin, 2001; 37: 772(周月明,佐佐健介,浅井滋生.金属学报, 2001;37:772) [12] Ye J T, Liu Z R, Xu S X, W Z. Hydrodynamics. Shanghai: Fudan University Press, 1989: 345(叶敬棠,柳兆荣,许世雄,吴正.流体力学.上海:复旦大学出版社, 1989:345) [13] Li T J, Sassa K, Asai S. Acta Metall Sin, 1997; 33: 971(李廷举,佐佐健介,浅井滋生.金属学报, 1997;33:971) [14] Chen F, Duan Z L, Wang W A. Experiments of Material Mechanics. Wuhan: Huazhong University of Science & Technology Press, 1999: 133(陈锋,段自力,王文安.材料力学实验.武汉:华中理工大学出版社, 1999:133) [15] Zhang X Y, Qi B M, Zhu X L. Applied Chemic Handbook. Beijing: National Defence Industry Press, 1986: 322(张向宇,戚保民,朱鑫林.实用化学手册.北京:国防工业出版社, 1986:322) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|