| 304不锈钢在室温下非比例应力和应变循环变形行为实验研究 |
| 杨显杰 高庆 蔡力勋 刘宇杰 |
| 西南交通大学应用力学与工程系; 成都 610031 |
|
| An Experimental Study on the Deformation Behavior of SS304 Stainless Steel UnderNonproportional Cyclic Stress and Strain at Room Temperature |
| YANG Xianjie; GAO Qing; CAI Lixun; LIU Yujie |
| Department of Applied Mechanics and Engineering; Southwest Jiaotong University; Chengdu 610031 |
引用本文:
杨显杰; 高庆; 蔡力勋; 刘宇杰 . 304不锈钢在室温下非比例应力和应变循环变形行为实验研究[J]. 金属学报, 2004, 40(9): 935-942 .
,
,
,
.
An Experimental Study on the Deformation Behavior of SS304 Stainless Steel UnderNonproportional Cyclic Stress and Strain at Room Temperature[J]. Acta Metall Sin, 2004, 40(9): 935-942 .
[1] Ikegami K, Niitsu Y. Nuclear Eng Design, 1989; 114: 355 [2] Murakami S, Kawai M, Ohmi Y. J Eng Mater Technol-Trans ASME, 1989; 111: 278 [3] McDowell D L. J Eng Mater Technol-Trans, 1985; 107:307 [4] Tanaka E, Murakami S, Ooka M. J Mech Phys Solids,1985; 33: 559 [5] Yang X J. J Eng Mater Technol-Trans ASME, 1997; 119:12 [6] Yang X J, Gao Q, He G Q, Cai L X. Ada Metall Sin,1996; 32: 15(杨显杰,高庆,何国求,蔡力勋.金属学报,1996;32:15) [7] Hassan T, Kyriakides S. Int J Plast, 1994; 10: 185 [8] Jiang Y, Sehitoglu H. Int J Plast, 1994; 10: 579 [9] McDowell D L. Int J Plast, 1995; 11: 397 [10] Delobelle P, Robinet P, Bocher L. Int J Plast, 1995; 11:295 [11] Corona E, Hassan T, Kyriakides S. Int J Plast, 1996; 12:117 [12] Yang X J, Gao Q, Cai L X, Xiang Y K. Ada Aeronaut Astronaut Sin, 1997; 18: 395(杨显杰,高庆,蔡力勋,向阳开.航空学报,1997;18:395) [13] Yang X J, Gao Q, Cai L X, Xiang Y K. Ada Mech SolidsSin, 1997; 10: 359 [14] Ohno N, Abdel-Karim M, Kobayashi M, Igari T. Int JPlast, 1998; 14: 355 [15] Bower A F. J Mech Phys Solids, 1989; 37: 455 [16] Yang X J. PhD thesis, Southwest Jiaotong University,Chengdu, 1992(杨显杰.西南交通大学博士学位论文,成都, 1992)< |
|