| 约束条件下界面纯铝层裂尖应力场的数值分析 |
| 韩礼红 李梁 孙军 |
| 西安交通大学金属材料强度国家重点实验室; 西安 710049 |
|
| Numerical Analysis of the Crack-Tip Stress Field in Pure Aluminum Sheet Constrained by Interfaces |
| HAN Lihong; LI Liang; SUN Jun |
| State Key Laboratory for Mechanical Behavior of Materials; Xi'an Jiaotong University; Xi'an 110049 |
引用本文:
韩礼红; 李梁; 孙军 . 约束条件下界面纯铝层裂尖应力场的数值分析[J]. 金属学报, 2004, 40(9): 920-926 .
,
,
.
Numerical Analysis of the Crack-Tip Stress Field in Pure Aluminum Sheet Constrained by Interfaces[J]. Acta Metall Sin, 2004, 40(9): 920-926 .
[1] Tolle M C, Kassner M E. Ada Me.ta.ll Mater, 1995; 43:287 [2] Kassner M E, Kennedy T C, Schrems K K. Acta Mater,1998; 46: 6445 [3] Dalgleish B J, Trumble K P, Evans A G. Acta Metall,1989; 37: 1923 [4] Rosen R S, Kassner ME. J Vac Sci Technol, 1990; 8: 19 [5] Klassen R J, Weatherly G C, Ramaswami B. Metall Trans,1992; 23A: 3281 [6] Li M, Soboyejo W O. Metall Mater Trans, 2000; 31A: 1385 [7] Sun J, Boyd J D. Int J Press Ves Pip, 2000; 77: 369 [8] Varias A G, Suo Z, Shih C F. J Mech Phys Solids, 1991;39: 963 [9] Lin G Y, Kim Y J, Cornec A, Schwalbe K H. Comput Mater Sci, 1997; 9: 36 [10] Kim Y J, Lin G Y, Cornec A, Brocks W, Schwalbe K H.Int J Fract, 1996; 75: R9 [11] Tvergaard V, Huang Y, Hutchinson J W. Eur J Mech,1992; 11A: 215 [12] Chen J H, Wang Q, Wang G Z, Li Z. Ada Mater, 2003;51: 1841 [13] Han L H, Li L, Sun J. Acta Metall Sin, 2003; 39: 920(韩礼红,李梁,孙军.金属学报,2003;39:920) [14] Sun J. PhD thesis, Xi'an Jiaotong University, 1989(孙军.西安交通大学博士学位论文, 1989) [15] Huang Y, Hutchinson J W, Tvergaard V. J Mech PhysSolids, 1991; 39: 223 [16] Hsia K J, Suo Z, Yang W. J Mech Phys Solids, 1994; 42:877 [17] Cook R F, Suo Z. MRS Bull, 2002; 27(1) : 45 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|