| Fe和两种工业钢在500℃含氯气氛中ZnCl2-KCl 盐膜下的腐蚀 |
| 张 轲 牛 焱 吴维tao |
| 中国科学院金属研究所金属腐蚀与防护国家重点实验室; 沈阳 110016 |
|
| CORROSION OF PURE IRON AND TWO COMMERCIAL STEELS BENEATH ZnCl2-KCl DEPOSITS IN A CONTROLLED ATMOSPHERE CONTAINING HCl AT 500℃ |
| ZHANG Ke; NIU Yan; WU Weitao |
| State Key Laboratory for Corrosion and Protection; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
张; 轲; 牛焱; 吴维tao . Fe和两种工业钢在500℃含氯气氛中ZnCl2-KCl 盐膜下的腐蚀[J]. 金属学报, 2004, 40(4): 388-392 .
,
,
,
.
CORROSION OF PURE IRON AND TWO COMMERCIAL STEELS BENEATH ZnCl2-KCl DEPOSITS IN A CONTROLLED ATMOSPHERE CONTAINING HCl AT 500℃[J]. Acta Metall Sin, 2004, 40(4): 388-392 .
[1] Spiegel M. Mater Corros, 1999; 50: 373 [2] Li Y S, Niu Y, Liu G, Wu W T. Corros Sci Prot Technol, 2000; 12: 224(李远士,牛 焱,刘 刚,吴维(?).腐蚀科学与防护技术,2000;12:224) [3] Wright I G, Krause H H. ASME Research Report, CRTD-Vol.38, the American Soc of Mech Eng, New York, 1996 [4] Otero E, Pardo A, Perez F J, Utrilla M V, Levi T. OxidMet, 1998; 49: 467 [5] Li Y S, Al-Omary M, Niu Y, Zhang K. High Temp MaterPro, 2002; 21: 11 [6] Shinata Y, Nishi Y. Oxid Met, 1986; 26: 201 [7] Kim A S, McNallan M J. Corros, 1990; 46:746 [8] Zahs A, Spiegel M, Grabke H J. Corros Sci, 2000; 42:1093 [9] Li Y S, Niu Y, Liu G, Wu W T. Acta Metall Sin, 2000;36: 1183(李远士,牛 焱,刘 刚,吴维(?).金属学报,2000;36:1183) |
|