| 半固态Al-6.5Si合金的流变特性 |
| 陈金玉 鞠丽平 李亮 |
| 沈阳师范大学物理系110034 |
|
引用本文:
陈金玉; 鞠丽平; 李亮 . 半固态Al-6.5Si合金的流变特性[J]. 金属学报, 2003, 39(5): 476-481 .
[1] Kirkwood D H. Int Mater Rev, 1994; 39: 173 [2] Flemings M C. Metall Trans, 1991; 22A: 957 [3] Fan Z. Int Mater Rev, 2002; 47: 49 [4] Joly P A, Mehrabian R. J Mater Sci, 1976; 11: 1393 [5] Wang N, Shu G, Yang J. Mater Trans JIM, 1990; 31: 715 [6] Kattamis T Z, Piccone T J. Mater Sci Eng, 1991; A131:265 [7] Turng L S, Wang K K. J Mater Sci, 1991; 26: 12173 [8] Loue W R, Landkroon S, Kool W H. Mater Sci Eng, 1992;9: 241 [9] Mada M, Ajersch F. Mater Sci Eng, 1996; A212: 157 [10] Mada M, Ajersch M. Mater Sci Eng, 1996; A212: 171 [11] Modigell M, Koke J. In: Bhasin A K eds., Proc 5th Int Conf on Semi-Solid Processing Of Alloys and Composites,Colorado School of Mines, 1998: 417 [12] Modigell M, Koke J. Mechan Time-Depend Mater, 1999;3: 15 [13] Quaak C J, Katgerman L, Kool W H. In: Kirkwood D H, Kapranos P eds., Proc 4th Int Conf on Semi-Solid Processing of Alloys and Composites, The University of Sheffield, 1996: 35 [14] Kumar P, Martin C L, Brown S. Acta Metall Mater, 1994; 42: 3595 [15] Koke J, Modigell M. Proc Int Symp on Advanced Forming and Die Manufacturing Technology, Pusan, South Korea, 1999: 101 [16] Koke J, Modigell M, Peter J. Appl Mech Eng, 1999; 4: 345 [17] Burgos G R, Alexandrou A N. J Rheology, 1999; 43: 485 [18] Cross J. Colloid Sci, 1965; 20: 417 [19] Cheng D C H, Inter J. Cosmetic Sci, 1987; 9: 151 [20] Alexandrou A N, Burgos G R, Entov V M. In: Chiarmetta G J, Rosso M eds., Proc 6th Int Coof on Semi-Solid Processing of Alloys and Composites, Turin, Italy: Politenico di Torion, 2000: 553 [21] Kirkwood, Ward P J, Barkhudarov M, Chin S B, Atkinson H V, Liu Y. In: Chiarmetta G L, Rosso M eds., Proc 6th Int Coof on Semi-Solid Processing of Alloys and Composites, Turin, Italy: Politenico di Torion, 2000: 545 [22] Kumar P, Martin C L, Brown S. Metall Trans, 1993: 24A: 1107 [23] Chen J Y, Fan Z. Mater Sci Technol, 2002; 18: 237 [24] Fan Z, Chen J Y. Mater Sci Technol, 2002; 18: 243 [25] Chen J Y, Fan Z. Mater Sci Technol, 2002; 18: 250 [26] Fan Z, Chen J Y. Mater Sci Technol, 2002; 18: 258 [27] Sharma K C, Ferreira J H, Govender G, Damm O. In: Chiarmetta G L, Rosso M eds., Proc 6th Int Coof on Semi-Solid Processing of Alloys and Composites, Turin, Italy: Politenico di Torion, 2000: 253 [28] Kopper A, Apelian D. In: Chiarmetta G L, Rosso M eds., Proc 6th In t Coof on Semi-Solid Processing of Alloys and Composites, Turin, Italy: Politenico di Torion, 2000: 379 [29] Ito Y, Flemings M C, Cornie J A. In: Sekhar J A, Dantzig J A eds., Nature and Properties of Semi-Solid Materials, Warrendale, Pennsylvania: The Metals Society of AIME, 1991: 3 [30] Sigworth G K. Can Metall Q, 1996; 35: 101 [31] Suery M, Zavaliangos A. In: Chiarmetta G L, Rosso M eds., Proc 6th Int Coof on Semi-Solid Processing of Alloys and Composites, Turin, Italy: Politenico di Torion, 2000: 129 [32] Alexandrou A N, Burgos G R, Entov V M. In: Chiarmetta G L, Rosso M eds., Proc 6h Int Coof on Semi-Solid Processing of Alloys and Composites, Turin, Italy: Politenico di Torion, 2000: 161 [33] Burgos G R, Alexandrou A N, Entov V. J Mater Proc Technol, 2001; 110: 164 [34] Matin C L, Kumar P, Brown S. Acta Metall Mater, 1994; 42: 3603 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|