| 近熔点液态纯铁和Fe-C二元合金的微观结构 |
| 骆军;翟启杰;赵沛 |
| 上海大学材料科学与工程学院; 上海 200072; 中国科学院物理研究所; 北京 100080 |
|
| Microstructures of Liquid Pure Iron and Fe-C Alloy Near the Melting Point |
| LUO Jun; ZHAI Qijie; ZHAO Pei |
| School of Materials Science and Engineering; Shanghai University; Shanghai 200072;Institute of Physics the Chinese Academy of Science; Beijing 100080 |
引用本文:
骆军; 翟启杰; 赵沛 . 近熔点液态纯铁和Fe-C二元合金的微观结构[J]. 金属学报, 2003, 39(1): 5-9 .
,
,
.
Microstructures of Liquid Pure Iron and Fe-C Alloy Near the Melting Point[J]. Acta Metall Sin, 2003, 39(1): 5-9 .
[1] Bian X F. The Heredity of Casting Metal. Jinan: Publisher of Shandong Science and Technology, 1999: 1(边秀房.铸造金属遗传学.济南:山东科学技术出版社,1999:1) [2] Qin J Y, Bian X F, Wang W M, Sliousarenko S I, Xu C Y, Ma J J. Sci Chin (E), 1998; 28(2) : 97(秦敬玉,边秀房,王伟民, Sijusarenko S I,徐昌业,马家骥.中国科学(E辑),1998;28(2) :97) [3] Qin J Y, Bian X F, Wang W M, Sliousarenko S I, Xu CY, Ma J J. Sci Chin, 1998; 41E: 182 [4] Waseda Y. The Structure of Non-Crystalline Materials.New York: McGraw-Hill, 1980: 27 [5] Waseda Y, Shinoda K, Sugiyama K, Takeda S, TerashimaK, Toguri J M. J Appl Phys, 1995; 34(8A): 4124 [6] Xu S S. The development of X-ray diffraction. Beijing:Science publisher, 1986: 103(许顺生.X射线衍射学进展.北京:科学出版社,1986:103) [7] Maret M, Pasturel A, Senillou C, Dubois J M, Chieux P.J Phys Fr, 1989; 50: 295 [8] Qin J Y, Bian X F, Wang W M, Ma J Y, Xu C Y. ChinSci Bulletin, 1998; 43: 1445(秦敬玉,边秀房,王伟民,马家骥,徐昌业.科学通报,1998;43:1445) [9] Huang S T. The Structure and Structure Analysis of Amorphous Material. Beijing: Science Publisher, 1987: 10(黄胜涛著.非晶态材料的结构和结构分析.北京:科学出版社,1987:10) [10] Wang H R, Ye Y F, Wang W M, Qin J Y. Chin Sci Bulletin, 2000; 45: 1501(王焕荣,叶以富,王伟民,秦敬玉.科学通报,2000;45:1501) [11] Cervinka L. J Non-Cryst Solids, 1998; 232-234: 1 [12] Elliott S R. Nature, 1991; 354: 445( |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|