| 离心力作用下Al/SiCp系统二维凝固过程的数值模拟 |
| 杜卓林 陈义良 黄庆 章明宇 |
| 中国科学技术大学热科学与能源工程系;合肥230026 |
|
引用本文:
杜卓林; 陈义良; 黄庆; 章明宇 . 离心力作用下Al/SiCp系统二维凝固过程的数值模拟[J]. 金属学报, 2002, 38(4): 359-364 .
[1] Kang S G, Rohatgi C S, Narendranath C S, Cole G S.ISIJ Int, 1994; 34: 247 [2] Gao J W, Wang C Y. Mater Sci Eng, 2000; 292A: 207 [3] Stefanescu D M, Juretzko F R, Dhindaw B K, Catalina A,Sen S, Curreri P A. Metall Mater Trans, 1998; 29A: 1697 [4] Asthana S, Tewari S N. J Mater Sci, 1993; 28: 5414 [5] Ding J, Gidaspow D. Am Inst Chem Eng J,1990; 36: 523 [6] Gidaspow D. Appl Mech Rev, 1986; 39: 1 [7] Richardson J F, Zaki W N. Trans Inst Chem Eng, 1954;32: 35 [8] Spalding D B. In: Shih T M ed., Numerical Properties andMethodologies in Heat Transfer, Proc 2nd National Symp,Washington, DC: Hemisphere Publishing, 1985: 421 [9] Voller V R. Numer Heat Transfer, 1990: 17B: 155 |
|