用改进单纯形法优化钢的硬度与强度换算公式 |
缪宗华 李正红 |
福建农林大学交通工程系;南平353001 |
|
引用本文:
缪宗华; 李正红 . 用改进单纯形法优化钢的硬度与强度换算公式[J]. 金属学报, 2001, 37(5): 543-546 .
[1] Editorial Board of Handbook of Mechanical Engineering.Handbook of Mechanical Engineering(3). 2nd ed, Beijing:Machinery Industry Press, 1996: 4 (机械工程手册编委会.机械工程手册(3).第2版,北京:机械工业出版社,1996:4) [2] He Z M, Hong W. Sci Silvesinicae, 1993; 29: 558 (何宗明,洪伟.林业科学,1993; 29:558) [3] Editorial Board of Handbook of Heat Treatment. Handbook of Heat Treatment(4). Beijing: Machinery IndustryPress, 1978: 141 (热处理手册编委会.热处理手册(4).北京:机械工业出版社,1978:141) [4] Yu B H. Computer Design for Steels. Beijing: Metallurgical Industry Press, 1996: 10 (余柏海.钢的计算机设计,北京:冶金工业出版社,1996:10) [5] Zhu X Q. Handbook of Practical Metal Material. Vol.1,Shanghai: Shanghai Science and Technology Press, 1993:45 (祝燮权.实用金属材料手册.第1卷,上海:上海科技出版社,1993:45) |
|