| FeMoSiB纳米晶薄带的裂纹扩展阻力和结构的关系 |
| 甘阳 周本濂 |
| 中国科学院金属研究所;沈阳110016 |
|
引用本文:
甘阳; 周本濂 . FeMoSiB纳米晶薄带的裂纹扩展阻力和结构的关系[J]. 金属学报, 2001, 37(4): 391-394 .
[1] Sui M L, Patu S, He Y Z. Scr Metall Mater 1991; 25:1537 [2] Olofinjana A O, Kern J H, Davies H A. Mater Lett, 1994;20: 5 [3] Olofinjana A O, Davies H A. Nanostruct Mater 1995; 6:465 [4] Gan Y, Zhou B L. Acta Metall Sin, 2000; 36; 356(甘阳,周本濂.金属学报, 2000; 36: 356) [5] Liu X D, Wang J T, Ding B Z. Scr Metall Mater 1993;28: 59 [6] Tetelman A S, McEvily A J. Fracture of Structural Materials. New York: Wiley, 1967: 138 [7] McMahon C J Jr, Vitek B, Kameda J. In: Chell G Ged., Fracture Mechanics, Vol.2, Parking, Essex: AppliedScience, 1981: 193 [8] Rice R W. J Mater Sci, 1996; 31: 1969 [9] Ping D H, Li D X, Ye H Q, Liu X D, Hu Z Q. Mater SciEng, 1995; 195A: 211K |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|