|
|
|
| Al-Ti-B合金中TiB2和AlB2的从头算研究 |
| 李喜珍 边秀房 李秀军 刘相法 |
| 山东大学材料液态结构及其遗传性教育部重点实验室;济南250061 |
|
引用本文:
李喜珍; 边秀房; 李秀军; 刘相法 . Al-Ti-B合金中TiB2和AlB2的从头算研究[J]. 金属学报, 2001, 37(3): 235-238 .
[1] Abdel-Hamid A A. Z Metallkde, 1989; 34: 247 [2] Jones G P, Pearson J. Metall Trans, 1976; 7B: 223 [3] McCartney D G. Int Mater Rev, 1989; 34: 247 [4] Birch M E J, Fisher P. Aluminium Technology, London:The Institute of Metals, 1986: 117 [5] Guzowaski M M, Sigworth G K, Sentner D A. MetallTrans, 1987; 18A: 603 [6] Spittle J A, Sadli S. Cast Metals, 1995; 7: 247 [7] Birch M E J, Cowed A J J. Solidification Processing, London: The Institute of Metals, 1988: 149 [8] McElvany S W, Cassady C J J. Phys Chem, 1990; 94: 2057 [9] Chevel R, Hirrien M, Sergent M. Polyhedron, 1986; 5: 87 [10] Mitchell P C H, Wear 1984; 100: 281 [11] Chianell R R. Catal Rev-Sci Eng, 1984; 26: 361 [12] Becke A D. J Chem Phys, 1993; 98: 5648 [13] Becke A D. J Chem Phys, 1988; 88: 1053 [14] Kohn W, Sham L J. Phys Rev, 1965; 140: 1133 [15] Lee C, Yang W, Pars R G. Phys Rev, 1988; 37B: 785 [16] Becke D A. Phys Rev, 1988; 38: 3 098 [17] Miehlich B, Savin A, Stoll H, Preuss H. Chem Phys Lett,1989; 157: 200 [18] McGartney D G. Int Mater Rev,1989; 34: 247m |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|