| NiAl微晶涂层对NiAl-TiC复合材料高温氧化性能的影响 |
| 杨松岚 王福会 |
| 中国科学院金属腐蚀与防护研究所金属腐蚀与防护国家重点实验室; 沈阳110015 |
|
引用本文:
杨松岚; 王福会 . NiAl微晶涂层对NiAl-TiC复合材料高温氧化性能的影响[J]. 金属学报, 2000, 36(9): 985-989 .
[1] Miracle D B. Acta Metall Mater,1993; 41: 649 [2] Vedula K, Pathave V, Aslanidis I, TiTran R H. Mat ResSoc Symp Proc,1986; 39: 411 [3] Vedula K, Stephens J R. Mat Res Soc Symp Proc, 1987;81: 381 [4] Kumar K S, Whittenberger J D. Moter Sci Technol,1992;8: 317 [8] Whittenberger J D, Viswanadham R K, Mannan S K,Sprissler B. J Mater Sci, 1990; 25: 35 [6] Wang L, Aresenault R J. Mater Sci Egg, 1990; A127: 91 [7] Whittenberger J D, Kumar K S, Mannan S K. Mater HighTemp,1991; 9: 3 [8] Alman D E, Stoloff N S. Int J Powder Metall , 1991; 27:29 [9] Xing Z P, Dai J Y, Guo J T, An G Y, Hu Z Q. ScriptaMetall Mater, 1994; 31: 1141 [10] Xing Z P, Yu L G, Guo J T, J,Dai Y, An G Y, Ha ZQ. J Mater Sci Lett, 1995; 14: 443 [11] Baker i, Munroe P R. J Met, 1988; 40: 28 [12] Xing Z P, Guo J T, Han Y F, Yu L G. Metall Moter Trans,1997; 28A: 1079 [13] Guo J T, Xing Z P, Wang S H, Li H. J Iron Steel Res,1997; 9: 23(郭建亭.邢占平,王淑荷,李辉.钢铁研究学报增刊.1997;9:23) [14] Xing Z P, Guo J T, Hu Z Q, An G Y. Acta Metall Sin,1994; 7: 45 [15] Xing Z P, Yu L G, Guo J T, Dai J Y, An G Y, Hu Z Q.'J Mater Sci Lett, 1996; 14: 443 [16] Jiang D T. Doctoral Thesis, Institute of Metal Research,The Chinese Academy of Sciences, Shenyang,1998: 12(姜东涛.博士学位论文,中国科学院金属研究所,沈阳,1998:12) [17] TIng Z L, Wang F H, Wu W T. Oxid Met, 1997; 48: 511 [18] Yang S L, Wang F H. Acta Metall Sin, 2000; 36: 511(杨松岚,王福会.金属学报,2000;36:511) [19] Gesmundo F, Viani F, Niu Y, Douglass D L. Oxid Met,1994; 39:197 [20] Gesmundo F, Viani F, Niu Y. Oxid Met,1994; 42: 285 [21] Gesmundo F, Viani F, Niu Y, Douglas. D L. Oxid Met,1994; 42: 409 [22] Gesmundo F, Viani F, Niu Y. Oxid Met, 1994; 42: 465 [23] Niu Y, Gesmundo F, Viani F, Wu W T. Oxid Met, 1997;47: 21 [24] Rahmal A, Spencer P J. Oxid Met, 1991; 35: 53 [25] Backer S, Rahmel A, Schorr M, Schutze M. Oxid Met,1992; 38: 425 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|