| 异质焊头Cr5Mo/Cr21Ni12碳扩散的研究 |
| 黄明亮 于承志 |
| 大连理工大学材料工程系; 大连 116024 |
|
引用本文:
黄明亮; 于承志 . 异质焊头Cr5Mo/Cr21Ni12碳扩散的研究[J]. 金属学报, 2000, 36(9): 902-906 .
[1] Lundin C D. Welding J, 1982; 61: 58s [2] Pavlovsky J, Million B, Ciha K, Stransky K. Mater SciEng,1991; 149A: 105 [3] He K S, Cao X F. Welding of Dissimilar Metal. Beijing:Mechanical Industry Press, 1986: 43(何康生,曹雄夫.异种金属焊接.北京:机械工业出版社,1986: 43) [4] Huang M L. Thesis of Master's Degree, Dalian Universityof Technology, 1995: 56(黄明亮.硕士学位论文,大连: 大连理工大学, 1995: 56) [5] Titchmarsh J M. In: Sturgess J M ed. Proc 9th IntCongress on Electron Microscopy. Toronto:The Micro- scopical Society of Canada, 1978: 618 [6] Pilling J, Ridley N. Metall Trans, 1982; 13A: 557 [7] Crank J. The mathematics of Diffusion. Oxford: Claren-don Press, 1975: 104 [8] Wang X T. Metal Materials. Beijing: Mechanical industry Press, 1987: 17(王笑天. 金属材料学. 北京:机械工业出版社,1987: 17) [9] Hillert M. Li Q B trans. Diffusive phase transformationand thermodynamics of alloys. Shenyang: Liaoning Sci-ence and Technology Press, 1984: 144(Hillert M. 李清斌译.合金中的扩散性相变与合金热力学.沈阳: 辽宁科学技术出版社,1984: 144) [10] Lu G X, Hou Z S. Physical Metallurgy.Shanghai: Shanghai Science and Technology Press, 1985: 271(卢光熙, 侯增寿. 金属学.上海: 上海科学技术出版社, 1985:271)V |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|